Bars and extruded sections of aluminium-copper-silicon-magnesium alloy (Solution treated and aged at room temperature) (Not exceeding 200 mm diameter or minor sectional dimension) (Cu 1.5, Si 1, Mg 0.8)

PSZJBL

Bibliographic Details
Main Author: 8096 British Standards Institution
Format:
Subjects:
_version_ 1796716765278896128
author 8096 British Standards Institution
author_facet 8096 British Standards Institution
author_sort 8096 British Standards Institution
collection OCEAN
description PSZJBL
first_indexed 2024-03-05T05:54:32Z
format
id KOHA-OAI-TEST:348327
institution Universiti Teknologi Malaysia - OCEAN
last_indexed 2024-03-05T05:54:32Z
record_format dspace
spelling KOHA-OAI-TEST:3483272020-12-19T17:12:02ZBars and extruded sections of aluminium-copper-silicon-magnesium alloy (Solution treated and aged at room temperature) (Not exceeding 200 mm diameter or minor sectional dimension) (Cu 1.5, Si 1, Mg 0.8) 8096 British Standards Institution PSZJBLBars (Engineering)Aluminum-copper-magnesium-silicon alloys
spellingShingle Bars (Engineering)
Aluminum-copper-magnesium-silicon alloys
8096 British Standards Institution
Bars and extruded sections of aluminium-copper-silicon-magnesium alloy (Solution treated and aged at room temperature) (Not exceeding 200 mm diameter or minor sectional dimension) (Cu 1.5, Si 1, Mg 0.8)
title Bars and extruded sections of aluminium-copper-silicon-magnesium alloy (Solution treated and aged at room temperature) (Not exceeding 200 mm diameter or minor sectional dimension) (Cu 1.5, Si 1, Mg 0.8)
title_full Bars and extruded sections of aluminium-copper-silicon-magnesium alloy (Solution treated and aged at room temperature) (Not exceeding 200 mm diameter or minor sectional dimension) (Cu 1.5, Si 1, Mg 0.8)
title_fullStr Bars and extruded sections of aluminium-copper-silicon-magnesium alloy (Solution treated and aged at room temperature) (Not exceeding 200 mm diameter or minor sectional dimension) (Cu 1.5, Si 1, Mg 0.8)
title_full_unstemmed Bars and extruded sections of aluminium-copper-silicon-magnesium alloy (Solution treated and aged at room temperature) (Not exceeding 200 mm diameter or minor sectional dimension) (Cu 1.5, Si 1, Mg 0.8)
title_short Bars and extruded sections of aluminium-copper-silicon-magnesium alloy (Solution treated and aged at room temperature) (Not exceeding 200 mm diameter or minor sectional dimension) (Cu 1.5, Si 1, Mg 0.8)
title_sort bars and extruded sections of aluminium copper silicon magnesium alloy solution treated and aged at room temperature not exceeding 200 mm diameter or minor sectional dimension cu 1 5 si 1 mg 0 8
topic Bars (Engineering)
Aluminum-copper-magnesium-silicon alloys
work_keys_str_mv AT 8096britishstandardsinstitution barsandextrudedsectionsofaluminiumcoppersiliconmagnesiumalloysolutiontreatedandagedatroomtemperaturenotexceeding200mmdiameterorminorsectionaldimensioncu15si1mg08