Anisotropy magnetoresistance differential probe for characterization of sub-millimeter surface defects on galvanized steel plate
Defects such as cracks can cause dangerous damage to the metal structure and may lead to structural collapses. Cracks can exist in various shapes and sizes where they can start to develop from small scale lower than 1 mm and spread to contribute to the complete fracture of components. Hence, early d...
Main Authors: | Nurul A’in, Nadzri, Mohd Mawardi, Saari, Mohd Aufa Hadi, Putera Zaini, Aiman, Mohd Halil, M., Ishak, Tsukada, Keiji |
---|---|
Format: | Article |
Language: | English |
Published: |
Sage
2021
|
Subjects: | |
Online Access: | http://umpir.ump.edu.my/id/eprint/31735/1/Anisotropy%20magnetoresistance%20differential%20probe%20for%20characterization%20of%20sub-millimeter%20surface.pdf |
Similar Items
-
Characterization of sub-millimeter backside-slit defects on galvanized steel plates using a phase-sensitive AMR gradiometer and low excitation frequency
by: Mohd Mawardi, Saari, et al.
Published: (2020) -
An MFL probe using shiftable magnetization angle for front and back side crack evaluation
by: Mohd Aufa Hadi, Putera Zaini, et al.
Published: (2019) -
Evaluation of back-side slits with sub-millimeter resolution using a differential AMR probe
by: M. A. H. P., Zaini, et al. -
Detection of crack on a mild steel plate by using a magnetic probe incorporating an array of fluxgate sensors
by: Mohd Aufa Hadi, Putera Zaini, et al.
Published: (2023) -
Development of ect probe for back side crack evaluation
by: Nurul A’in, Nadzri, et al.
Published: (2020)