On Post-Weld Heat Treatment of a Single Crystal Nickel-Based Superalloy Joint by Linear Friction Welding
Three types of post-weld heat treatment (PWHT), i.e. solution treatment + primary aging + secondary aging (I), secondary aging (II), and primary aging + secondary aging (III), were applied to a single crystal nickel-based superalloy joint made with linear friction welding (LFW). The results show t...
Main Authors: | T. J. Ma, Y. H. Yang, W. Y. Li, Y. Zhang, M. Yan |
---|---|
Format: | Article |
Language: | English |
Published: |
Eastern Macedonia and Thrace Institute of Technology
2015-09-01
|
Series: | Journal of Engineering Science and Technology Review |
Subjects: | |
Online Access: | http://www.jestr.org/downloads/Volume8Issue6/fulltext86112015.pdf |
Similar Items
-
Oxidation behaviors of the rotary friction welded joints of HT700 superalloy in saturated water steam at 700 ℃
by: Chunlin Huang, et al.
Published: (2022-06-01) -
The effect of inclusions and pores on creep crack propagation of linear friction welded joints of GH4169 superalloy
by: Xiawei Yang, et al.
Published: (2024-03-01) -
Analysis of microstructural evolution and mechanical properties of FGH101 powder superalloy and IN718 deformed superalloy via inertia friction welding
by: Jun Zhou, et al.
Published: (2025-01-01) -
Rotary Friction Welding of Inconel 718 to Inconel 600
by: Ateekh Ur Rehman, et al.
Published: (2021-02-01) -
Effect of heat input on microstructure and mechanical properties of laser welded joint of Inconel 617 nickel-based superalloy
by: CHENG Hao, et al.
Published: (2023-01-01)