Geochemistry of Fe3+ in the hydrothermal dickite from Jedlina Zdroj (Lower Silesia, Poland)
Geochemical analysis for Fe was made on a representative sample of dickite-rich hydrothermal clay from Jedlina Zdroj. The mineralogy of the sample is comparatively simple, dickite being the principal component (>95 wt. % of the total sample), with lesser amounts of goethite and barite. Geochemica...
Main Authors: | , , , , |
---|---|
Format: | Article |
Language: | English |
Published: |
Serbian Chemical Society
2009-01-01
|
Series: | Journal of the Serbian Chemical Society |
Subjects: | |
Online Access: | http://www.doiserbia.nb.rs/img/doi/0352-5139/2009/0352-51390912477P.pdf |
Summary: | Geochemical analysis for Fe was made on a representative sample of dickite-rich hydrothermal clay from Jedlina Zdroj. The mineralogy of the sample is comparatively simple, dickite being the principal component (>95 wt. % of the total sample), with lesser amounts of goethite and barite. Geochemical fractionation and inductively coupled plasma-optical emission spectrometry indicated that most of the Fe (ca. 97 wt. % of the total metal) resides in the dickite. Electron spin resonance showed that some of the Fe in the dickite structure is in the form of Fe3+. A substantial proportion of these ions (as well as Fe) in the dickite matrix were probably contained in the original hydrothermal dickite-forming solution. From the geochemistry of Fe3+, it was deduced that the oxidation potential (Eh) and pH of the solution during the formation of dickite from the Jedlina Zdroj were approximately 0.45-0.95 V (highly oxygenated) and 0-4 (highly acidic), respectively. |
---|---|
ISSN: | 0352-5139 1820-7421 |