The electrical properties of wollastonite inlaid NR/SBR type elastomer based material have been evaluated. Electrical properties of the samples were measured in the temperature range of 303 to 453 K and the frequency range of 100 Hz – 40 MHz. All electrically measured parameters were given anomalies...

Full description

Bibliographic Details
Main Authors: E. Şentürk, T. Yüksel, M. Okutan, A. Demirer, N. Akçakale, İ. Okur
Format: Article
Language:English
Published: University of Chemistry and Technology, Prague 2012-07-01
Series:Ceramics-Silikáty
Subjects:
Online Access:http://www.ceramics-silikaty.cz/2012/pdf/2012_02_145.pdf
Description
Summary:The electrical properties of wollastonite inlaid NR/SBR type elastomer based material have been evaluated. Electrical properties of the samples were measured in the temperature range of 303 to 453 K and the frequency range of 100 Hz – 40 MHz. All electrically measured parameters were given anomalies at 385 K. Only one type of dielectric relaxation process have been observed for all measurements. Physical parameters characterizing the dielectric behavior have been obtained by fitting the experimental results in the modified Debye equation. The activation energy which is thermally activated by dielectric relaxation process have been calculated to be 0.58 eV. DC conductivity increasing by temperature has been explained with the help of VFT model whereas the AC one has been clarified by the OLPT model.
ISSN:0862-5468
1804-5847