Corrosion Activity Laser Treated Aluminum-12% Silicon Alloy with Fe and Ti Powders at Two Different Energies
In This work, the corrosion activity of laser treated almium-12%silicon alloy was tested. The addition of Fe and Ti as elemental powders was studied. Two different laser energies of 750 and 1000 kJ were used. Corrosion measurements by potential static at 3mV.sec-1in condensed synthetic automotive so...
Main Author: | Mervit Hanoos |
---|---|
Format: | Article |
Language: | English |
Published: |
Unviversity of Technology- Iraq
2018-11-01
|
Series: | Engineering and Technology Journal |
Subjects: | |
Online Access: | https://etj.uotechnology.edu.iq/article_175311_bc74bb9c28b54afc9f40fa5020d31df2.pdf |
Similar Items
-
Distinctive localized corrosion behavior of β-Mg2Si and α-Al(Fe,Mn)Si phases in a 6082 alloy
by: Y.H. Gao, et al.
Published: (2024-03-01) -
Corrosion of aluminum and aluminum alloys /
by: Davis, J. R. (Joseph R.)
Published: (1999) -
Effect of Ti and Sn additions on mechanical properties of Aluminum- Silicon - copper alloy
by: Israa A. Alkadir
Published: (2016-12-01) -
Effects of Ni and Co on the Corrosion Resistance of Al-Si-Cu-Zn-Fe Alloys in NaCl Solution
by: Marcella G. C. Xavier, et al.
Published: (2022-04-01) -
Effect of Cu as a Minority Alloying Element on the Corrosion Behaviour of Amorphous and Crystalline Al-Ni-Si Alloy
by: Vanya Dyakova, et al.
Published: (2023-08-01)