Pitting Corrosion Behavior of 304 SS and 316 SS Alloys in Aqueous Chloride and Bromide Solutions
The importance of the present work falls on the pitting corrosion behavior investigation of 304 SS and 316 SS alloys in 3.5 wt% of aqueous solution bearing with chloride and bromide anion at different solutions temperature range starting from (20-50)oC due to the pitting corrosion tremendous effec...
Main Authors: | Ibtehal Kareem Shakir, Abdul-Kareem Mohammed Ali Alsamurraee, Shaymaa Mahdi Saleh |
---|---|
Format: | Article |
Language: | English |
Published: |
University of Baghdad
2018-01-01
|
Series: | Journal of Engineering |
Online Access: | https://www.jcoeng.edu.iq/index.php/main/article/view/494/421 |
Similar Items
-
Pitting Corrosion Behavior of 304 SS and 316 SS Alloys in Aqueous Chloride and Bromide Solutions
by: Ibtehal Kareem Shakir, Ass. Prof. Dr., et al.
Published: (2018-01-01) -
Analysis of Corrosion of Hastelloy-N, Alloy X750, SS316 and SS304 in Molten Salt High-Temperature Environment
by: Ketan Kumar Sandhi, et al.
Published: (2021-01-01) -
Effect of HAc on the Metastable Pitting Corrosion of 304 SS in NaCl Solution
by: Hanlu Zhang, et al.
Published: (2022-05-01) -
Comparison of passivation behavior of SS316L with that of SS304 in tritiated water solution
by: M. Oyaidzu, et al.
Published: (2016-12-01) -
Synergistic effect of crevice corrosion and galvanic coupling on 304SS fasteners degradation in chloride environments
by: Enobong Felix Daniel, et al.
Published: (2023-02-01)