Effect of hydrogenation disproportionation conditions on magnetic anisotropy in Nd-Fe-B powder prepared by dynamic hydrogenation disproportionation desorption recombination
Various anisotropic Nd-Fe-B magnetic powders were prepared by the dynamic hydrogenation disproportionation desorption recombination (d-HDDR) treatment with different hydrogenation disproportionation (HD) times (tHD). The resulting magnetic properties and microstructural changes were investigated. Th...
Main Authors: | Masao Yamazaki, Takashi Horikawa, Chisato Mishima, Masashi Matsuura, Nobuki Tezuka, Satoshi Sugimoto |
---|---|
Format: | Article |
Language: | English |
Published: |
AIP Publishing LLC
2017-05-01
|
Series: | AIP Advances |
Online Access: | http://dx.doi.org/10.1063/1.4975697 |
Similar Items
-
Effects of Water Quenching Before Hydrogenation, Disproportionation, Desorption, and Recombination Process on the Magnetic Properties of Nd-Fe-B Powder
by: Sri Bimo Pratomo, et al.
Published: (2016-04-01) -
Crystallographic alignment in the recombination stage in d-HDDR process of Nd-Fe-B-Ga-Nb powders
by: Takashi Horikawa, et al.
Published: (2016-05-01) -
Design of High-Remanence Nd-Fe-B Hot-Pressed Magnets by Manipulating Coercivity of Hydrogenation-Disproportionation-Desorption-Recombination Treated Anisotropic Precursors
by: Jae-Gyeong Yoo, et al.
Published: (2023-12-01) -
Effect of Redox Potential on Diiron-Mediated Disproportionation of Hydrogen Peroxide
by: Patrik Török, et al.
Published: (2023-03-01) -
Structural dissection of the maltodextrin disproportionation cycle of the arabidopsis plastidial disproportionating enzyme 1 (DPE1)
by: O'Neill, E, et al.
Published: (2015)