Effect of Different Decontamination Procedures for Saliva-Contaminated Uncured Bonding Agent on Shear Bond Strength of Composite to Enamel

Background and Aim: Prevention of contamination during the procedural steps is a req-uisite for achieving a satisfactory composite restoration. The aim of this experimental study was to assess the shear bond strength of composite to enamel following two differ-ent decontamination procedures of saliv...

Full description

Bibliographic Details
Main Authors: Hossein Afshar, Shahram Mosharrafiyan, Samaneh Abbasi Salimkandi
Format: Article
Language:English
Published: Islamic Dental Association of Iran 2015-01-01
Series:Journal of Islamic Dental Association of Iran
Subjects:
Online Access:http://jidai.ir/browse.php?a_code=A-10-1-812&slc_lang=en&sid=1
Description
Summary:Background and Aim: Prevention of contamination during the procedural steps is a req-uisite for achieving a satisfactory composite restoration. The aim of this experimental study was to assess the shear bond strength of composite to enamel following two differ-ent decontamination procedures of saliva-contaminated uncured bonding agent in comparison with uncontaminated condition. Materials and Methods: Thirty-six extracted sound human premolars and incisors were selected. Enamel of the buccal surface was ground flat. The teeth were divided into 3 groups of 12 each. In the control group (1), 3M Single Bond adhesive was used according to the manufacturer’s instructions, without any contamination. In groups 2 and 3 un-cured adhesive was saliva contaminated and then: (group 2) rinsed, dried, etched (5 seconds), rinsed, dried and adhesive was reapplied and (group 3) cured, dried, etched (5 seconds), rinsed, dried and adhesive was reapplied. Then composite cylinders were bonded to the enamel surfaces. Finally, samples were sheared using Instron testing machine and shear bond strength data were subjected to one-way ANOVA. Results: The mean bond strength was 16.5317 MPa in the control group, 16.2308 MPa in rinsed contaminated bonding group and 15.8025 MPa in cured contaminated bonding group. No statistically significant difference was found in the mean shear bond strength of groups 1,2 and 3 (p=0.954). Conclusion: Both decontamination protocols (groups 2 and 3) resulted in acceptable bond strength and both were comparable with uncontaminated condition.