Effect of acid leaching conditions on impurity removal from silicon doped by magnesium
The effect of magnesium addition into a commercial silicon and its leaching refining behavior is studied for producing solar grade silicon feedstock. Two different levels of Mg is added into a commercial silicon and the leaching of the produced alloys by 10% HCl solution at 60 ℃ for different durati...
Main Authors: | Stine Espelien, Jafar Safarian |
---|---|
Format: | Article |
Language: | English |
Published: |
AIMS Press
2017-07-01
|
Series: | AIMS Energy |
Subjects: | |
Online Access: | http://www.aimspress.com/energy/article/1529/fulltext.html |
Similar Items
-
Influence of iron, aluminum, calcium, titanium and vanadium impurities removal from silicon based on Cu-catalyzed chemical leaching
by: Fengshuo Xi, et al.
Published: (2021-01-01) -
Kinetics of Magnesiothermic Reduction of Natural Quartz
by: Azam Rasouli, et al.
Published: (2022-09-01) -
Controlled preparation of silicon and magnesium silicide on silica glass substrate through magnesiothermic reduction
by: Takashi Henmi, et al.
Published: (2020-03-01) -
Magnesiothermic reduction of silica glass substrate—Chemical states of silicon in the generated layers
by: Yuki Tsuboi, et al.
Published: (2017-09-01) -
SILICON REFINING BY VACUUM TREATMENT
by: André Alexandrino Lotto, et al.
Published: (2014-12-01)