Extrusion limit diagram of Mg–5Bi–3Al–1Zn alloy and effects of extrusion parameters on its microstructures and mechanical properties

Hot-compressive tests and finite element simulations were carried out to construct an extrusion limit diagram of a Mg–5Bi–3Al–1Zn (wt.%) alloy in this work. It was observed that 310 °C became a dividing line, below which the safe extrusion zone was narrow because the stress required to induce the pl...