The importance of pre-treatment of spent hydrotreating catalysts on metals recovery
This work describes a three-step pre-treatment route for processing spent commercial NiMo/Al2O3 catalysts. Extraction of soluble coke with n-hexane and/or leaching of foulant elements with oxalic acid were performed before burning insoluble coke under air. Oxidized catalysts were leached with 9 mol...
Main Authors: | Alexandre Luiz de Souza Pereira, Cristiano Nunes da Silva, Júlio Carlos Afonso, José Luiz Mantovano |
---|---|
Format: | Article |
Language: | English |
Published: |
Sociedade Brasileira de Química
2011-01-01
|
Series: | Química Nova |
Subjects: | |
Online Access: | http://www.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40422011000100027&lng=en&tlng=en |
Similar Items
-
Recuperação de metais de catalisadores de hidrorrefino usados via fusão com KHSO4 Recovery of elements from spent hydrorefining catalysts after fusion with KHSO4
by: Julio Carlos Afonso, et al.
Published: (2006-07-01) -
A Review of Recovery of Palladium from the Spent Automobile Catalysts
by: Bin Xu, et al.
Published: (2022-03-01) -
Recovery and extraction of platinum from spent catalysts: A review
by: Somayeh Kolbadinejad, et al.
Published: (2023-06-01) -
Reciclagem química de zeólitas comerciais desativadas
by: Afonso Júlio Carlos, et al.
Published: (2004-01-01) -
Industrial-Scale Technology for Molybdic Acid Production from Waste Petrochemical Catalysts
by: Katarzyna Leszczyńska-Sejda, et al.
Published: (2023-08-01)