Flotation performances and surface properties of chalcopyrite with xanthate collector added before and after grinding

In this study, effects of the collector added before grinding and after grinding on the subsequent flotation and mineral surface properties were investigated. The pH was controlled at 10 during the grinding and flotation processes opened to the atmosphere. With enough amounts of sodium butyl xanthat...

Full description

Bibliographic Details
Main Authors: Huiqing Peng, Di Wu, Mohamed Abdelmonem
Format: Article
Language:English
Published: Elsevier 2017-01-01
Series:Results in Physics
Online Access:http://www.sciencedirect.com/science/article/pii/S2211379717314043
Description
Summary:In this study, effects of the collector added before grinding and after grinding on the subsequent flotation and mineral surface properties were investigated. The pH was controlled at 10 during the grinding and flotation processes opened to the atmosphere. With enough amounts of sodium butyl xanthate addition, adding the collector before grinding recovered more chalcopyrite than adding it after grinding in single mineral flotation. The Eh of each ground pulp before and after conditioning were measured and it was found that adding collector before grinding obtained higher and relatively suitable pulp potential for chalcopyrite flotation. Particle size analyses of the flotation products indicate that the different flotation recoveries occurred due to the different flotation losses in fine particles (<20 μm). XPS analyses focused on the fine particles of flotation feedings and found that more carbon and oxygen, and less iron were remained on mineral surfaces when the collector was added before grinding, due to the higher collector adsorption capacity, larger free oxygen adsorbance and less iron oxide/hydroxide species. Keywords: Grinding, Xanthate, Chalcopyrite flotation, XPS
ISSN:2211-3797