Influence of the Anodizing Time on the Microstructure and Immersion Stability of Tartaric-Sulfuric Acid Anodized Aluminum Alloys
Tartaric-sulfuric acid anodizing (TSA) has been selected by the aerospace industry to replace Cr(VI)-based anodizing treatments of aluminum alloys. Modification of the bath composition can result in the necessity to revise the process conditions, including the time necessary to obtain the desired pr...
Main Authors: | Florian Raffin, Jacques Echouard, Polina Volovitch |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2023-05-01
|
Series: | Metals |
Subjects: | |
Online Access: | https://www.mdpi.com/2075-4701/13/5/993 |
Similar Items
-
Electrochemical Noise Analysis Using Experimental Chaos Theory, Power Spectral Density and Hilbert–Huang Transform in Anodized Aluminum Alloys in Tartaric–Phosphoric–Sulfuric Acid Solutions
by: Cynthia Martínez-Ramos, et al.
Published: (2023-11-01) -
Changes in the Structure and Corrosion Protection Ability of Porous Anodic Oxide Films on Pure Al and Al Alloys by Pore Sealing Treatment
by: Haruno Yanagimoto, et al.
Published: (2022-11-01) -
Low Temperature Sealing of Anodized Aluminum Alloy for Enhancing Corrosion Resistance
by: Hyunbin Jo, et al.
Published: (2020-10-01) -
Corrosion of Titanium Alloys Anodized Using Electrochemical Techniques
by: Jesús Manuel Jáquez-Muñoz, et al.
Published: (2023-02-01) -
Nanoparticles deposition effects on 1050A aluminum alloy anodic layers
by: Gh A Gaber, et al.
Published: (2020-01-01)