Improved Strength of Peroxide-Bleached Deinked Pulp after TEMPO-Mediated Oxidation at Medium Consistency
Deinked pulp was pretreated using the 4-acetamido-2,2,6,6,- tetramethyl-pipelidine-1-oxyl radical (TEMPO)/NaBr/NaClO system and then bleached using hydrogen peroxide to achieve a medium pulp consistency. The effect of the amount of oxidant NaClO addition on the peroxide bleaching of deinked pulp was...
Main Authors: | , , , , |
---|---|
Format: | Article |
Language: | English |
Published: |
North Carolina State University
2015-08-01
|
Series: | BioResources |
Subjects: | |
Online Access: | http://ojs.cnr.ncsu.edu/index.php/BioRes/article/view/BioRes_10_4_6586_Hua_Improved_Strength_Peroxide_Bleached_Pulp |
_version_ | 1819064475933736960 |
---|---|
author | Feiguo Hua Shuhua Tong Rendang Yang Bin Wang Fei Yang |
author_facet | Feiguo Hua Shuhua Tong Rendang Yang Bin Wang Fei Yang |
author_sort | Feiguo Hua |
collection | DOAJ |
description | Deinked pulp was pretreated using the 4-acetamido-2,2,6,6,- tetramethyl-pipelidine-1-oxyl radical (TEMPO)/NaBr/NaClO system and then bleached using hydrogen peroxide to achieve a medium pulp consistency. The effect of the amount of oxidant NaClO addition on the peroxide bleaching of deinked pulp was studied. The treated pulp was characterized using X-ray diffraction (XRD) and scanning electron microscopy (SEM). The characterization of XRD and SEM showed that the treated pulp had a higher degree of crystallinity and more fibrillation than untreated pulp. Fiber quality analysis also revealed that the treated pulps had more fines and shorter fiber length than the untreated pulp. A handsheet test showed that the deinked pulps pretreated with the TEMPO system exhibited high tensile index values. The tensile index of the TEMPO pretreated pulp was 17% higher than that of the pulp bleached by hydrogen peroxide alone. |
first_indexed | 2024-12-21T15:31:10Z |
format | Article |
id | doaj.art-2c7095ba24764f30a4b206f29347b6d8 |
institution | Directory Open Access Journal |
issn | 1930-2126 1930-2126 |
language | English |
last_indexed | 2024-12-21T15:31:10Z |
publishDate | 2015-08-01 |
publisher | North Carolina State University |
record_format | Article |
series | BioResources |
spelling | doaj.art-2c7095ba24764f30a4b206f29347b6d82022-12-21T18:58:46ZengNorth Carolina State UniversityBioResources1930-21261930-21262015-08-011046586659610.15376/biores.10.4.6586-6596Improved Strength of Peroxide-Bleached Deinked Pulp after TEMPO-Mediated Oxidation at Medium ConsistencyFeiguo Hua0Shuhua Tong1Rendang Yang2Bin Wang3Fei Yang4School of Light Industry and Food Sciences, South China University of Technology; China Zhejiang Jinchang Paper Co., Ltd., Longyou, 324404, China; ChinaState Key Laboratory of Pulp and Paper Engineering, South China University of Technology, Guangzhou, 510640, China; ChinaState Key Laboratory of Pulp and Paper Engineering, South China University of Technology, Guangzhou, 510640, China; Key Laboratory of Pulp and Paper Science & Technology of Ministry of Education of China, Qilu University of Technology, Jinan, 250353, China; ChinaState Key Laboratory of Pulp and Paper Engineering, South China University of Technology, Guangzhou, 510640, China; Key Laboratory of Pulp and Paper Science & Technology of Ministry of Education of China, Qilu University of Technology, Jinan, 250353, China; ChinaDeinked pulp was pretreated using the 4-acetamido-2,2,6,6,- tetramethyl-pipelidine-1-oxyl radical (TEMPO)/NaBr/NaClO system and then bleached using hydrogen peroxide to achieve a medium pulp consistency. The effect of the amount of oxidant NaClO addition on the peroxide bleaching of deinked pulp was studied. The treated pulp was characterized using X-ray diffraction (XRD) and scanning electron microscopy (SEM). The characterization of XRD and SEM showed that the treated pulp had a higher degree of crystallinity and more fibrillation than untreated pulp. Fiber quality analysis also revealed that the treated pulps had more fines and shorter fiber length than the untreated pulp. A handsheet test showed that the deinked pulps pretreated with the TEMPO system exhibited high tensile index values. The tensile index of the TEMPO pretreated pulp was 17% higher than that of the pulp bleached by hydrogen peroxide alone.http://ojs.cnr.ncsu.edu/index.php/BioRes/article/view/BioRes_10_4_6586_Hua_Improved_Strength_Peroxide_Bleached_PulpDeinked pulpTEMPO/NaBr/NaClO systemHydrogen peroxide bleachingMedium consistency |
spellingShingle | Feiguo Hua Shuhua Tong Rendang Yang Bin Wang Fei Yang Improved Strength of Peroxide-Bleached Deinked Pulp after TEMPO-Mediated Oxidation at Medium Consistency BioResources Deinked pulp TEMPO/NaBr/NaClO system Hydrogen peroxide bleaching Medium consistency |
title | Improved Strength of Peroxide-Bleached Deinked Pulp after TEMPO-Mediated Oxidation at Medium Consistency |
title_full | Improved Strength of Peroxide-Bleached Deinked Pulp after TEMPO-Mediated Oxidation at Medium Consistency |
title_fullStr | Improved Strength of Peroxide-Bleached Deinked Pulp after TEMPO-Mediated Oxidation at Medium Consistency |
title_full_unstemmed | Improved Strength of Peroxide-Bleached Deinked Pulp after TEMPO-Mediated Oxidation at Medium Consistency |
title_short | Improved Strength of Peroxide-Bleached Deinked Pulp after TEMPO-Mediated Oxidation at Medium Consistency |
title_sort | improved strength of peroxide bleached deinked pulp after tempo mediated oxidation at medium consistency |
topic | Deinked pulp TEMPO/NaBr/NaClO system Hydrogen peroxide bleaching Medium consistency |
url | http://ojs.cnr.ncsu.edu/index.php/BioRes/article/view/BioRes_10_4_6586_Hua_Improved_Strength_Peroxide_Bleached_Pulp |
work_keys_str_mv | AT feiguohua improvedstrengthofperoxidebleacheddeinkedpulpaftertempomediatedoxidationatmediumconsistency AT shuhuatong improvedstrengthofperoxidebleacheddeinkedpulpaftertempomediatedoxidationatmediumconsistency AT rendangyang improvedstrengthofperoxidebleacheddeinkedpulpaftertempomediatedoxidationatmediumconsistency AT binwang improvedstrengthofperoxidebleacheddeinkedpulpaftertempomediatedoxidationatmediumconsistency AT feiyang improvedstrengthofperoxidebleacheddeinkedpulpaftertempomediatedoxidationatmediumconsistency |