Shape of a crack growth front under fatigue in the range of 106 - 107cycles
The paper explores the shape of a fatigue crack initiation in the interval of 106-107cycles of duplex stainless steel, commercially designated as SAF 2507. Particular emphasis is placed upon the development of the crack’s growth front and its subsequent expansion in three directions x, y, z. Created...
Main Author: | Georgi Georgiev Georgiev |
---|---|
Format: | Article |
Language: | English |
Published: |
Technical University of Varna, Bulgaria
2020-06-01
|
Series: | Annual Journal of Technical University of Varna |
Subjects: | |
Online Access: | https://aj-tuv.org/index.php/ajtuv/article/view/162 |
Similar Items
-
Influence of Heat Input on Microstructure and Mechanical Properties of Laser Weld Metal in 2507 Duplex Stainless Steel by Different Welding Speed and Welding Power
by: Shuai ZHAO, et al.
Published: (2024-02-01) -
Fatigue crack shape prediction based on vertex singularity
by: Hutař P., et al.
Published: (2008-11-01) -
Prediction of the Crack Front Shape of the Corner Interface Crack
by: Jelena M. Djoković, et al.
Published: (2023-11-01) -
Prediction of Shape Change for Fatigue Crack in a Round Bar Using Three-Parameter Growth Circles
by: Yali Yang, et al.
Published: (2019-04-01) -
Prediction of fatigue crack initiation life in SA312 Type 304LN austenitic stainless steel straight pipes with notch
by: A. Ramachandra Murthy, et al.
Published: (2022-05-01)