Zn-Mn-O: Ferromagnet at room temperature

Semiconductor Zn-Mn-O crystallites were synthesized by a solid state reaction method starting from the thermal decomposition of the appropriate oxalates. Samples were thermally treated in air at temperatures ranging from 400 to 900°C. The nominal concentrations of manganese werex = 0.01, 0.02, 0.04...