Microstructural and Mechanical Characterization of Al-0.80Mg-0.85Si-0.3Zr Alloy

In this study, Al-0.80Mg-0.85Si alloy was modified with the addition of 0.3 wt.-% zirconium and the variation of microstructural features and mechanical properties were investigated. In order to produce the billets, vertical direct chill casting method was used and billets were homogenized at 580 °C...