Kinetic of the surface dissolution of SAE-AISI 1005 steel in acid media
The automotive sector is one of the biggest consumers of ferrous materials, which require an efficient protection against corrosion. This protection can be reached applying adequate coatings. A careful surface preparation is required to apply any kind of coatings on surfaces. The surface preparation...
Main Authors: | Marina Magnani, Cecílio Sadao Fugivara, Roberto Garcia, Assis Vicente Benedetti |
---|---|
Format: | Article |
Language: | English |
Published: |
Universidade Estadual Paulista
2018-05-01
|
Series: | Eclética Química |
Online Access: | https://revista.iq.unesp.br/ojs/index.php/ecletica/article/view/538 |
Similar Items
-
On-site weld quality assessment and qualification for stainless steels tanks
by: Luis Henrique Guilherme, et al.
Published: (2022-07-01) -
Assessment of Charge Transport Through Barrier Membranes Before Application on Materials Surfaces
by: Jéssica Verger Nardeli, et al.
Published: (2022-09-01) -
Prediction of Bead Width In Submerged ArcWelding of Low Carbon Steel (AISI 1005)
by: Husham Jawad Kadhim, et al.
Published: (2015-02-01) -
Corrosion Behavior of an AISI/SAE Steel Cut by Electropulsing
by: Carlos Alberto Montilla, et al.
Published: (2019-11-01) -
1020 AISI-SAE steel Austenitic Nitrocarburising with alcohol and triethanolamine
by: Álvaro Castro P, et al.
Published: (2005-01-01)