The characteristics of μ phase precipitated during 720 °C long-term aging in alloy 617B
In this work, the precipitation of μ phase is detected in alloy 617B during 720 °C aging for 10 000 h. The lattice parameters of μ phase is determined as a = 0.4720–0.4760 nm and c = 2.5394–2.5656 nm in this work. The μ phase in alloy 617B is mainly composed of Mo and Cr, in accompany with Ni and Co...
Main Authors: | He Jiang, Jianxin Dong, Maicang Zhang |
---|---|
Format: | Article |
Language: | English |
Published: |
Elsevier
2019-04-01
|
Series: | Journal of Materials Research and Technology |
Online Access: | http://www.sciencedirect.com/science/article/pii/S223878541830591X |
Similar Items
-
Long-Exposure Air and Steam Oxidation Characteristics of IN 617 Alloys
by: Rishikesh Karthikeyan, et al.
Published: (2023-01-01) -
Influence of Dynamic Strain Aging on Tensile Deformation Behavior of Alloy 617
by: I.M.W. Ekaputra, et al.
Published: (2016-12-01) -
Low Cycle Fatigue Behaviors of Alloy 617 (INCONEL 617) Weldments for High Temperature Applications
by: Rando Tungga Dewa, et al.
Published: (2016-04-01) -
Creep Behavior of Diffusion-Welded Alloy 617
by: Injin Sah, et al.
Published: (2021-05-01) -
Microstructural characterization and mechanical properties of IN617 superalloy after long-term operation
by: mohsen mehdizadeh, et al.
Published: (2021-08-01)