Recovery of Diamond and Cobalt Powders from Polycrystalline Drawing Die Blanks via Ultrasound Assisted Leaching Process—Part 2: Kinetics and Mechanisms

The leaching of industrial polycrystalline diamond (PCD) blanks in aqua regia at atmospheric pressure between 60 °C and 80 °C was performed using an ultrasound to improve the rate of cobalt removal in order to be able to reuse very expensive polycrystalline diamond. Because cobalt (20 wt.%) is used...

ver descrição completa

Detalhes bibliográficos
Main Authors: Ferdinand Kießling, Srecko Stopic, Sebahattin Gürmen, Bernd Friedrich
Formato: Artigo
Idioma:English
Publicado em: MDPI AG 2020-06-01
Colecção:Metals
Assuntos:
Acesso em linha:https://www.mdpi.com/2075-4701/10/6/741