Summary: | The aim of the present study was to verify if there is any difference in the pulp chamber temperature rise during the photo-activation of two resin composites with different viscosities. Eighteen extracted bovine incisors were divided into two groups (n=9) that were restored with two different resin composites – Filtek Z250 and Filtek Flow (3M/ESPE Dental Products, St Paul, MN 55144, USA). During the photo-activation, with a conventional halogen light curing unit (XL 2500, 3M/ESPE), a type-K thermocouple registered the temperature rise peak in the pulp chamber. The temperature rise data were submitted to Student-t test at 5% significance. The resin composite Filtek Flow shows statically higher mean temperature rise (p<0.05). We conclude that the resin composites with different viscosities produce different temperature changes during the photo-activation.
|