Corrosion and Conservation Management of the Submarine HMAS AE2 (1915) in the Sea of Marmara, Turkey
The wreck site of the Australian First World War submarine HMAS AE2 in the Sea of Marmara had a salinity of 26‰ (parts per thousand) for the first 13 m, which increased to 41‰ at 21 m, after which it remained constant to the bottom at 72 m, where the dissolved oxygen was three...
Main Author: | Ian D. MacLeod |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2019-03-01
|
Series: | Heritage |
Subjects: | |
Online Access: | http://www.mdpi.com/2571-9408/2/1/58 |
Similar Items
-
Influence of cooling rate on the corrosion behavior of Al–Zn–In–Mg–Ag sacrificial anode
by: Yasi Zhang, et al.
Published: (2024-05-01) -
Design and Application of an In Situ Test Device for Rheological Characteristic Measurements of Liquefied Submarine Sediments
by: Hong Zhang, et al.
Published: (2021-06-01) -
Sedimentation in submarine canyons, fans, and trenches /
by: Stanley, Daniel Jean, et al.
Published: (1978) -
Influence of silicon on the corrosion behavior of Al–Zn–In sacrificial anode
by: G.F. Sperandio, et al.
Published: (2021-11-01) -
Cathodic Protection of Carbon Steel Using Aluminum as Sacrificial Anode in Sea Water
by: Muayad Fadhil Hamad
Published: (2015-01-01)