Color stability of nano-filled, micro-hybrid, and silorane-based dental composite resin materials
Aim: The purpose of this study was to investigate the color stability of nano-hybrid, micro-hybrid, and silorane-based composite resin restorative materials upon exposure to staining agents. Materials and Methods: One hundred twenty composites samples were prepared, 40 from each composite material...
Main Authors: | , |
---|---|
Format: | Article |
Language: | English |
Published: |
Wolters Kluwer Medknow Publications
2016-01-01
|
Series: | Saudi Journal of Oral Sciences |
Subjects: | |
Online Access: | http://www.saudijos.org//article.asp?issn=1658-6816;year=2016;volume=3;issue=1;spage=42;epage=48;aulast=ALShetili |
_version_ | 1819021085183574016 |
---|---|
author | Mohsen Saud M ALShetili Mohammad Al-Omari |
author_facet | Mohsen Saud M ALShetili Mohammad Al-Omari |
author_sort | Mohsen Saud M ALShetili |
collection | DOAJ |
description | Aim: The purpose of this study was to investigate the color stability of nano-hybrid, micro-hybrid, and silorane-based composite resin restorative materials upon exposure to staining agents.
Materials and Methods: One hundred twenty composites samples were prepared, 40 from each composite material (Filtek ® Z350, Filtek ® P90, and Filtek ® Z250). The specimens were randomly divided into four groups (10 of each sample). The specimens were incubated for 24 h in distilled water and then for 72 h in corresponding mediums (distilled water, red grape juice, green tea, coffee). The color of all the specimens was assessed before and after exposure with a spectrophotometer and total color change (ΔE) was calculated using ΔEFNx01 = [(ΔLFNx01)2 + (ΔaFNx01)2 + (ΔbFNx01)2]1/2. The data were analyzed with one-way analysis of variance (ANOVA) and Kolmogorov-Smirnov and the means of the solutions were compared by Tukey′s honestly significant difference (HSD) (P < 0.05).
Result: The lowest dicoloration was observed in Filtek ® LS P90 but it was not significant while the most discoloration was observed in Filtek ® Z350 and Filtek ® Z250. Also, coffee showed a highly significant (P > 0.05) discoloration compared with other media.
Conclusions: Within the limitations of this study, it may be concluded that silorane-based composites are more resistant to discoloration than bis-GMA-based composites and coffee had the highest effect on composite discoloration compared to other media. |
first_indexed | 2024-12-21T04:01:29Z |
format | Article |
id | doaj.art-63cacc1083d346d0b69312cb037b07c1 |
institution | Directory Open Access Journal |
issn | 1658-6816 |
language | English |
last_indexed | 2024-12-21T04:01:29Z |
publishDate | 2016-01-01 |
publisher | Wolters Kluwer Medknow Publications |
record_format | Article |
series | Saudi Journal of Oral Sciences |
spelling | doaj.art-63cacc1083d346d0b69312cb037b07c12022-12-21T19:16:42ZengWolters Kluwer Medknow PublicationsSaudi Journal of Oral Sciences1658-68162016-01-0131424810.4103/1658-6816.174336Color stability of nano-filled, micro-hybrid, and silorane-based dental composite resin materialsMohsen Saud M ALShetiliMohammad Al-OmariAim: The purpose of this study was to investigate the color stability of nano-hybrid, micro-hybrid, and silorane-based composite resin restorative materials upon exposure to staining agents. Materials and Methods: One hundred twenty composites samples were prepared, 40 from each composite material (Filtek ® Z350, Filtek ® P90, and Filtek ® Z250). The specimens were randomly divided into four groups (10 of each sample). The specimens were incubated for 24 h in distilled water and then for 72 h in corresponding mediums (distilled water, red grape juice, green tea, coffee). The color of all the specimens was assessed before and after exposure with a spectrophotometer and total color change (ΔE) was calculated using ΔEFNx01 = [(ΔLFNx01)2 + (ΔaFNx01)2 + (ΔbFNx01)2]1/2. The data were analyzed with one-way analysis of variance (ANOVA) and Kolmogorov-Smirnov and the means of the solutions were compared by Tukey′s honestly significant difference (HSD) (P < 0.05). Result: The lowest dicoloration was observed in Filtek ® LS P90 but it was not significant while the most discoloration was observed in Filtek ® Z350 and Filtek ® Z250. Also, coffee showed a highly significant (P > 0.05) discoloration compared with other media. Conclusions: Within the limitations of this study, it may be concluded that silorane-based composites are more resistant to discoloration than bis-GMA-based composites and coffee had the highest effect on composite discoloration compared to other media.http://www.saudijos.org//article.asp?issn=1658-6816;year=2016;volume=3;issue=1;spage=42;epage=48;aulast=ALShetiliColorcompositemicro-hybridsiloranenano-filled |
spellingShingle | Mohsen Saud M ALShetili Mohammad Al-Omari Color stability of nano-filled, micro-hybrid, and silorane-based dental composite resin materials Saudi Journal of Oral Sciences Color composite micro-hybrid silorane nano-filled |
title | Color stability of nano-filled, micro-hybrid, and silorane-based dental composite resin materials |
title_full | Color stability of nano-filled, micro-hybrid, and silorane-based dental composite resin materials |
title_fullStr | Color stability of nano-filled, micro-hybrid, and silorane-based dental composite resin materials |
title_full_unstemmed | Color stability of nano-filled, micro-hybrid, and silorane-based dental composite resin materials |
title_short | Color stability of nano-filled, micro-hybrid, and silorane-based dental composite resin materials |
title_sort | color stability of nano filled micro hybrid and silorane based dental composite resin materials |
topic | Color composite micro-hybrid silorane nano-filled |
url | http://www.saudijos.org//article.asp?issn=1658-6816;year=2016;volume=3;issue=1;spage=42;epage=48;aulast=ALShetili |
work_keys_str_mv | AT mohsensaudmalshetili colorstabilityofnanofilledmicrohybridandsiloranebaseddentalcompositeresinmaterials AT mohammadalomari colorstabilityofnanofilledmicrohybridandsiloranebaseddentalcompositeresinmaterials |