Characterization of fire behaviors associated with a thermal runaway in large-scale commercial LiNi0.8Co0.1Mn0.1O2/graphite cells under external ignition
The fire behaviors of large-format commercial batteries at varying states of charge (SOCs) under an external ignition source were experimentally studied. The thermal runaway of the battery mainly starts in the temperature interval of 470.1–526.5 K. The trigger time and temperature of the thermal run...
Main Authors: | Zhi Wang, Qingjie Zhao, Bo Yin, Haoran Zhai, Jian Wang, Weiguang An |
---|---|
Format: | Article |
Language: | English |
Published: |
Elsevier
2023-07-01
|
Series: | Case Studies in Thermal Engineering |
Subjects: | |
Online Access: | http://www.sciencedirect.com/science/article/pii/S2214157X2300432X |
Similar Items
-
Effects of Degradation on the Thermal Stability LiNi0.8Co0.1Mn0.1O2/Graphite Batteries
by: Takao INOUE, et al.
Published: (2022-11-01) -
Cycle-induced interfacial degradation and transition metal cross-over in LiNi0.8Mn0.1Co0.1O2-graphite cells
by: Bjorklund, E, et al.
Published: (2022) -
Carbonized Polymer Dots Enhancing Interface Stability of LiNi0.8Co0.1Mn0.1O2 Cathodes
by: Lin Li, et al.
Published: (2023-07-01) -
Ti4+ Substitution on Structure and Conductivity of LiNi0.8Mn0.1Co(0.1-x)TixO2 as Battery Cathode (x = 0.01, 0.02, and 0.03)
by: Maya Puspitasari Izaak, et al.
Published: (2022-12-01) -
Benchmarking the electrochemical parameters of the LiNi0.8Mn0.1Co0.1O2 positive electrode material for Li-ion batteries
by: Aleksandra A. Savina, et al.
Published: (2023-12-01)