Mechanical parameters of thermally modified ash wood determined on compression in tangential direction
Mechanical parameters of ash wood (Fraxinus excelsior) subjected to compression in tangential direction, before and after its thermal modification and measured at the moisture content close to the equilibrium moisture content of wood used inside and outside the house, (4 and 12%) were compared. Th...
Main Authors: | Waldemar Moliński, Edward Roszyk, Aleksander Jabłoński, Jakub Puszyński, Janusz Cegieła |
---|---|
Format: | Article |
Language: | English |
Published: |
Universidad del Bío-Bío
2018-04-01
|
Series: | Maderas: Ciencia y Tecnología |
Subjects: | |
Online Access: | https://revistas.ubiobio.cl/index.php/MCT/article/view/3075 |
Similar Items
-
Mechanical parameters of thermally modified ash wood determined by compression in radial direction
by: Waldemar Moliński, et al.
Published: (2016-10-01) -
Variation in Mechanical Properties within Individual Annual Rings in the Resonance Spruce Wood (Picea abies (L.) Karst.)
by: Waldemar Moliński, et al.
Published: (2014-09-01) -
Identification and characterization of the fungus Dothiorella sarmentorum on necrotic shoots of declining ash in Slovakia
by: Ivanová Helena
Published: (2018-05-01) -
Germination, Growth and Seedling Quality Index of Common Ash in
Immature and Mature Seed
by: M. Soleymanpour, et al.
Published: (2021-05-01) -
Perception of gravity expressed by production of cambial callus in ash (Fraxinus excelsior L) internodes
by: Ewa U. Kurczyńska, et al.
Published: (2011-01-01)