Sintering behavior and mechanism of tungsten powders prepared by solution combustion synthesis combined with hydrogen reduction
Nanosized tungsten powders were fabricated by solution combustion synthesis combined with hydrogen reduction. The powder had a size of 20 nm but possessed a large numbers of lattice defects. The fracture surface images at different temperatures show that the as-synthesized tungsten powder could be s...
Main Authors: | Tianhao Zhang, Pengqi Chen, Wen Yang, Xiaodong Zhang |
---|---|
Format: | Article |
Language: | English |
Published: |
IOP Publishing
2021-01-01
|
Series: | Materials Research Express |
Subjects: | |
Online Access: | https://doi.org/10.1088/2053-1591/ac19e8 |
Similar Items
-
Effect of Al2O3 addition on the sintering behavior of nano tungsten powder
by: Cheng-min SONG, et al.
Published: (2020-07-01) -
Some features of sintering of tungsten powders
by: Andreiev Igor Viktorovich, et al.
Published: (2016-01-01) -
Effect of jet milling processing on microstructure and mechanical properties of the sintered tungsten powders
by: LI Xing-yu, et al.
Published: (2021-06-01) -
Activated sintering of Tungsten heavy alloy
by: Chaurasia Jitender, et al.
Published: (2017-01-01) -
Effect of Ball Milling Parameters on Properties of Nano-Sized Tungsten Powder via Mechanochemical Processing
by: Feng Li, et al.
Published: (2024-09-01)