Q&P Response of a Medium Carbon Low Alloy Steel

An Fe-0.44%C-1.8%Si-1.3%Mn-0.82%Cr-0.28%Mo steel was subjected to quenching followed by low-temperature tempering (Q&T) and quenching and partitioning (Q&P) processing after full austenitization. The Q&P treatment led to an increase in the volume fraction of retained austenite (RA) by fa...

Full description

Bibliographic Details
Main Authors: Roman Mishnev, Yuliya Borisova, Sergey Gaidar, Tatiana Kniaziuk, Olga Vagina, Rustam Kaibyshev
Format: Article
Language:English
Published: MDPI AG 2023-03-01
Series:Metals
Subjects:
Online Access:https://www.mdpi.com/2075-4701/13/4/689