Sifat fisika dan analisis gugus fungsi karet seal o-ring dari bahan termoplastik elastomer nitrile butadiene rubber (NBR) dan polyvinyl chloride (PVC)

The purpose of this research was to determine the physical properties and functional groups on O-ring rubber seals made of thermoplastic elastomers blend NBR and PVC. Composition of the NBR / PVC were successively varied : 90/10; 85/15; 80/20; 75/25; 70/30 and 65/35 phr. Mixing process between NB...

Full description

Bibliographic Details
Main Authors: Arum Yuniari, Nursamsi Sarengat
Format: Article
Language:English
Published: Center for Leather, Rubber, and Plastics 2013-06-01
Series:Majalah Kulit, Karet, dan Plastik
Subjects:
Online Access:http://ejournal.kemenperin.go.id/mkkp/article/view/215/189
_version_ 1819048929716600832
author Arum Yuniari
Nursamsi Sarengat
author_facet Arum Yuniari
Nursamsi Sarengat
author_sort Arum Yuniari
collection DOAJ
description The purpose of this research was to determine the physical properties and functional groups on O-ring rubber seals made of thermoplastic elastomers blend NBR and PVC. Composition of the NBR / PVC were successively varied : 90/10; 85/15; 80/20; 75/25; 70/30 and 65/35 phr. Mixing process between NBR/PVC with additive used a two roll mill within a temperature of 60º - 80 ºC, the vulcanization process used a hydraulic press at a temperature of 170 oC and pressure of 150 kg/cm2. The physical properties were evaluated including tensile strength, elongation at break, hardness, before and after aging, hardness after immersion in isooctane and swelling while analysis of functional groups was also carried out by method of Fourier Transform Infrared Spectrophotometer (FTIR). The result of the best vulcanized was characterized by tensile strength 188.93 kg/cm2, the change of tensile strength after aging 2.50%, elongation at break of 400%, the change of elongation at break after aging was 12.5%, hardness 75 shore A, the change of hardness after aging 0%, the change of hardness after immersion in isooctane 1.3%, swelling 0.8% and functional group of vulcanisate was indicated by new peak (OH) at wave band of 3468 cm-1. Those formula met the requirements of the technical specifications of ASTM D 2000 seal O-ring.
first_indexed 2024-12-21T11:24:04Z
format Article
id doaj.art-75e1fca916fa48c2a7f49c8e131fcb44
institution Directory Open Access Journal
issn 1829-6971
2460-4461
language English
last_indexed 2024-12-21T11:24:04Z
publishDate 2013-06-01
publisher Center for Leather, Rubber, and Plastics
record_format Article
series Majalah Kulit, Karet, dan Plastik
spelling doaj.art-75e1fca916fa48c2a7f49c8e131fcb442022-12-21T19:05:42ZengCenter for Leather, Rubber, and PlasticsMajalah Kulit, Karet, dan Plastik1829-69712460-44612013-06-01291213010.20543/mkkp.v29i1.215Sifat fisika dan analisis gugus fungsi karet seal o-ring dari bahan termoplastik elastomer nitrile butadiene rubber (NBR) dan polyvinyl chloride (PVC)Arum Yuniari0Nursamsi Sarengat1Balai Besar Kulit, Karet dan PlastikBalai Besar Kulit, Karet dan PlastikThe purpose of this research was to determine the physical properties and functional groups on O-ring rubber seals made of thermoplastic elastomers blend NBR and PVC. Composition of the NBR / PVC were successively varied : 90/10; 85/15; 80/20; 75/25; 70/30 and 65/35 phr. Mixing process between NBR/PVC with additive used a two roll mill within a temperature of 60º - 80 ºC, the vulcanization process used a hydraulic press at a temperature of 170 oC and pressure of 150 kg/cm2. The physical properties were evaluated including tensile strength, elongation at break, hardness, before and after aging, hardness after immersion in isooctane and swelling while analysis of functional groups was also carried out by method of Fourier Transform Infrared Spectrophotometer (FTIR). The result of the best vulcanized was characterized by tensile strength 188.93 kg/cm2, the change of tensile strength after aging 2.50%, elongation at break of 400%, the change of elongation at break after aging was 12.5%, hardness 75 shore A, the change of hardness after aging 0%, the change of hardness after immersion in isooctane 1.3%, swelling 0.8% and functional group of vulcanisate was indicated by new peak (OH) at wave band of 3468 cm-1. Those formula met the requirements of the technical specifications of ASTM D 2000 seal O-ring.http://ejournal.kemenperin.go.id/mkkp/article/view/215/189O-ring rubber sealsNBRPVCphysical propertiesfunctional group
spellingShingle Arum Yuniari
Nursamsi Sarengat
Sifat fisika dan analisis gugus fungsi karet seal o-ring dari bahan termoplastik elastomer nitrile butadiene rubber (NBR) dan polyvinyl chloride (PVC)
Majalah Kulit, Karet, dan Plastik
O-ring rubber seals
NBR
PVC
physical properties
functional group
title Sifat fisika dan analisis gugus fungsi karet seal o-ring dari bahan termoplastik elastomer nitrile butadiene rubber (NBR) dan polyvinyl chloride (PVC)
title_full Sifat fisika dan analisis gugus fungsi karet seal o-ring dari bahan termoplastik elastomer nitrile butadiene rubber (NBR) dan polyvinyl chloride (PVC)
title_fullStr Sifat fisika dan analisis gugus fungsi karet seal o-ring dari bahan termoplastik elastomer nitrile butadiene rubber (NBR) dan polyvinyl chloride (PVC)
title_full_unstemmed Sifat fisika dan analisis gugus fungsi karet seal o-ring dari bahan termoplastik elastomer nitrile butadiene rubber (NBR) dan polyvinyl chloride (PVC)
title_short Sifat fisika dan analisis gugus fungsi karet seal o-ring dari bahan termoplastik elastomer nitrile butadiene rubber (NBR) dan polyvinyl chloride (PVC)
title_sort sifat fisika dan analisis gugus fungsi karet seal o ring dari bahan termoplastik elastomer nitrile butadiene rubber nbr dan polyvinyl chloride pvc
topic O-ring rubber seals
NBR
PVC
physical properties
functional group
url http://ejournal.kemenperin.go.id/mkkp/article/view/215/189
work_keys_str_mv AT arumyuniari sifatfisikadananalisisgugusfungsikaretsealoringdaribahantermoplastikelastomernitrilebutadienerubbernbrdanpolyvinylchloridepvc
AT nursamsisarengat sifatfisikadananalisisgugusfungsikaretsealoringdaribahantermoplastikelastomernitrilebutadienerubbernbrdanpolyvinylchloridepvc