Evolution of interfacial structure of the joints between a tungsten-copper composite and austenitic stainless steel
Joining of CuW70 composite and 0Cr18Ni9 stainless steel was successfully achieved at temperatures 1150 °C with durations from 15 to 90 min after adding a pure copper intermediate layer. Microstructure, phase composition and elemental distribution at the interfacial region were studied. The optimum j...
Main Authors: | Youting Huang, Yuanfei Zha, Xiaolong Zhou, Xiaowei Li, Wei Li, Qiaohang Guo, Wenzhe Chen, Dongliang Peng |
---|---|
Format: | Article |
Language: | English |
Published: |
IOP Publishing
2021-01-01
|
Series: | Materials Research Express |
Subjects: | |
Online Access: | https://doi.org/10.1088/2053-1591/abd731 |
Similar Items
-
Effects of Electromagnetic Stirring on the Cast Austenitic Stainless Steel Weldments by Gas Tungsten Arc Welding
by: Sheng-Long Jeng, et al.
Published: (2018-08-01) -
Austenitic stainless steels : microstructure and mechanical properties
by: 314170 Marshall, P.
Published: (1984) -
Creep characteristics of austenitic stainless steel foil at elevated temperature /
by: Ilya Izyan Shahrul Azhar, 1988-, et al.
Published: (2013) -
Creep characteristics of austenitic stainless steel foil at elevated temperature [electronic resource] /
by: Ilya Izyan Shahrul Azhar, 1988-
Published: (2013) -
Impact energy of austenitic stainless steel at low temperature /
by: 488032 Muhammad Shukri Ab. Rashid, et al.
Published: (2007)