Corrosion of a chimney liner operated for 130,000 hours
The tests were carried out for a coal-fired boiler heating a single-family house with a floor area of 220 m2. The tests concerned the chimney lining (structure and surface layer - produced oxides/deposits), hard coal (eco-pea coal) and furnace ash. The chimney liner was located in a chimney made of...
Main Author: | |
---|---|
Format: | Article |
Language: | English |
Published: |
University of Belgrade, Technical Faculty, Bor
2023-01-01
|
Series: | Journal of Mining and Metallurgy. Section B: Metallurgy |
Subjects: | |
Online Access: | https://doiserbia.nb.rs/img/doi/1450-5339/2023/1450-53392300023G.pdf |
_version_ | 1826818808296243200 |
---|---|
author | Gwoździk M. |
author_facet | Gwoździk M. |
author_sort | Gwoździk M. |
collection | DOAJ |
description | The tests were carried out for a coal-fired boiler heating a single-family house with a floor area of 220 m2. The tests concerned the chimney lining (structure and surface layer - produced oxides/deposits), hard coal (eco-pea coal) and furnace ash. The chimney liner was located in a chimney made of bricks joined with concrete. A chimney liner made of austenitic steel was tested. The chimney liner was operated for 130,000 hours. The chimney insert was studied on the inside and outside each cross-section. Coal with a grain size of 5–21 mm was analyzed. The bottom ash consisted of both loose ash and a mass of glassy sintered ash, the so-called slag. The thorough examinations of the examined materialsincludec: microscopic examinations with a VHX-7000 digital microscope and Jeol JSM-6610LV scanning electron microscopes. Chemical composition analysis by energy dispersive X-ray spectroscopy (EDS) in conjunction with the scanning electron microscopy (SEM) was performed. The surface topography (roughness) was measured with a VHX microscope using a Gaussian filter. Based on the tests, the following parameters were determined: arithmetic mean height, maximum height, height of the highest peak, depth of the lowest depression, root mean square height, skewness, kurtosis. |
first_indexed | 2024-03-09T00:07:16Z |
format | Article |
id | doaj.art-7fcbb6a131504bf89b4db2d16cd9b3d3 |
institution | Directory Open Access Journal |
issn | 1450-5339 2217-7175 |
language | English |
last_indexed | 2025-02-16T05:58:42Z |
publishDate | 2023-01-01 |
publisher | University of Belgrade, Technical Faculty, Bor |
record_format | Article |
series | Journal of Mining and Metallurgy. Section B: Metallurgy |
spelling | doaj.art-7fcbb6a131504bf89b4db2d16cd9b3d32025-02-03T07:48:35ZengUniversity of Belgrade, Technical Faculty, BorJournal of Mining and Metallurgy. Section B: Metallurgy1450-53392217-71752023-01-0159226927710.2298/JMMB230206023G1450-53392300023GCorrosion of a chimney liner operated for 130,000 hoursGwoździk M.0Czestochowa University of Technology, Faculty of Production Engineering and Materials Technology, Department of Materials Engineering, Czestochowa, PolandThe tests were carried out for a coal-fired boiler heating a single-family house with a floor area of 220 m2. The tests concerned the chimney lining (structure and surface layer - produced oxides/deposits), hard coal (eco-pea coal) and furnace ash. The chimney liner was located in a chimney made of bricks joined with concrete. A chimney liner made of austenitic steel was tested. The chimney liner was operated for 130,000 hours. The chimney insert was studied on the inside and outside each cross-section. Coal with a grain size of 5–21 mm was analyzed. The bottom ash consisted of both loose ash and a mass of glassy sintered ash, the so-called slag. The thorough examinations of the examined materialsincludec: microscopic examinations with a VHX-7000 digital microscope and Jeol JSM-6610LV scanning electron microscopes. Chemical composition analysis by energy dispersive X-ray spectroscopy (EDS) in conjunction with the scanning electron microscopy (SEM) was performed. The surface topography (roughness) was measured with a VHX microscope using a Gaussian filter. Based on the tests, the following parameters were determined: arithmetic mean height, maximum height, height of the highest peak, depth of the lowest depression, root mean square height, skewness, kurtosis.https://doiserbia.nb.rs/img/doi/1450-5339/2023/1450-53392300023G.pdfchimney inserteco-pea coalaustenitic steel |
spellingShingle | Gwoździk M. Corrosion of a chimney liner operated for 130,000 hours Journal of Mining and Metallurgy. Section B: Metallurgy chimney insert eco-pea coal austenitic steel |
title | Corrosion of a chimney liner operated for 130,000 hours |
title_full | Corrosion of a chimney liner operated for 130,000 hours |
title_fullStr | Corrosion of a chimney liner operated for 130,000 hours |
title_full_unstemmed | Corrosion of a chimney liner operated for 130,000 hours |
title_short | Corrosion of a chimney liner operated for 130,000 hours |
title_sort | corrosion of a chimney liner operated for 130 000 hours |
topic | chimney insert eco-pea coal austenitic steel |
url | https://doiserbia.nb.rs/img/doi/1450-5339/2023/1450-53392300023G.pdf |
work_keys_str_mv | AT gwozdzikm corrosionofachimneylineroperatedfor130000hours |