Investigation of the 0.4C-35Cr-45Ni-Nb Alloy after Service in High-Temperature Steam and Hydrocarbons Environment
The paper presents the results of investigation of the 0.4C-35Cr-45Ni-Nb alloy, which operated in the cracked hydrocarbon feeds and dilution steam at 1125 °C. The material originated from the pyrolytic furnace coil tubes, of which internal walls were in contact with the aforementioned medium, wherea...
Main Authors: | Juliusz Orlikowski, Michał Szociński, Janusz Zygmuntowicz, Gabriel Gajewski, Wojciech Filipkowski, Kazimierz Darowicki |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2021-10-01
|
Series: | Materials |
Subjects: | |
Online Access: | https://www.mdpi.com/1996-1944/14/20/6139 |
Similar Items
-
Study on the adsorption of Cr (VI) and Cr (III) species on activated carbon in water samples collected from industrial landfill areas by spectrometry (ICP-MS, GFAAS) and energy despersive x-ray fluorescence (EDXRF) /
by: Alias Mohd. Yusof, 1951-2014, et al.
Published: (2002) -
Principles of combustion in the steam boiler furnace/
by: 222542 Pratt, Arthur Deudney
Published: (1936) -
Thermal Behavior and Kinetics of Shenmu Coal Pyrolyzed under Hydrogen-Rich or Methane-Gas-Rich Atmosphere
by: Chong Zou, et al.
Published: (2023-02-01) -
Influence of processing parameters on dehydrogenation of TiH2 in the preparation of Ti–Nb: A review
by: Anis Fatehah Sa'aidi, et al.
Published: (2022-11-01) -
Genetic mechanism of pyrolytically desorbed hydrocarbon
by: Guangzhi LI, et al.
Published: (2021-07-01)