Ecologically friendly construction is impossible without the use of materials that are characterized by a low emission of dangerous substances from the surface and have other appropriate properties. A solution of the problem related to the elaboration of special measures taken to reduce the emission...

Full description

Bibliographic Details
Main Authors: Shabanova Galina, Korohodska Alla, Shumejko Vita
Format: Article
Language:English
Published: EDP Sciences 2017-01-01
Series:MATEC Web of Conferences
Online Access:https://doi.org/10.1051/matecconf/201711601014
Description
Summary:Ecologically friendly construction is impossible without the use of materials that are characterized by a low emission of dangerous substances from the surface and have other appropriate properties. A solution of the problem related to the elaboration of special measures taken to reduce the emission of ammonia from construction materials and the structures manufactured using the Portland cement has been offered. An optimized composite dope was developed and optimized for the Portland cement composition that contains the nitric acid calcium, which is one of the ingredients that can considerably reduce the concentration of nitrogencontaining compounds, making thus the construction materials less dangerous to the human health. Strength characteristics of the cement stone with the composite dope were studied and it was established that a level of the intensification of a gain in the strength is rather significant and by the seventh day the hardening exceeds the values peculiar for the dope-free compositions at an age of 28 days by more than 45 %.
ISSN:2261-236X