Caracterización eléctrica de disoluciones sólidas (Cr,V,Ti)O<sub>2</sub> con estructura rutilo

In this work (Cr,V,Ti)O2 solid solutions with rich-TiO2 compositions have been synthesized. Green samples and samples after each calcination have been characterized by X-Ray diffraction at room temperature, UV-V spectroscopy and electronic microscopy, in order to confirm the stability of these solid...

Full description

Bibliographic Details
Main Authors: Monrós, G., Tena, M. A., Badenes, J. A., Benet, P., Calbo, J., Llusar, M., Sorlí, S.
Format: Article
Language:English
Published: Elsevier 2004-08-01
Series:Boletín de la Sociedad Española de Cerámica y Vidrio
Subjects:
Online Access:http://ceramicayvidrio.revistas.csic.es/index.php/ceramicayvidrio/article/view/432/450
_version_ 1818510324559511552
author Monrós, G.
Tena, M. A.
Badenes, J. A.
Benet, P.
Calbo, J.
Llusar, M.
Sorlí, S.
author_facet Monrós, G.
Tena, M. A.
Badenes, J. A.
Benet, P.
Calbo, J.
Llusar, M.
Sorlí, S.
author_sort Monrós, G.
collection DOAJ
description In this work (Cr,V,Ti)O2 solid solutions with rich-TiO2 compositions have been synthesized. Green samples and samples after each calcination have been characterized by X-Ray diffraction at room temperature, UV-V spectroscopy and electronic microscopy, in order to confirm the stability of these solid solutions with rutile-type structure at high temperatures (1400ºC). With the calcined samples at 1400ºC pellets were presses and Seebeck coefficient and complex impedance spectroscopy measurements were done. In these materials, the electrical behaviour corresponds to a extrinsic p-type semiconduction. The electrical conductivity is higher than that obtained in V-TiO2 solid solutions and it is enhanced with the amount of dopants in the TiO2 matrix.<br><br>En este estudio se han sintetizado disoluciones sólidas (Cr,V,Ti)O2 con composiciones ricas en TiO2. Las muestras, crudas y después de cada calcinación, se han caracterizado a temperatura ambiente por difracción de rayos X, espectroscopia UV-V y microscopía eléctronica para confirmar la estabilidad de estas disoluciones sólidas con estructura rutilo a altas temperaturas (1400 ºC). Se han prensado pastillas con las muestras calcinadas a 1400 ºC y con ellas se han realizado medidas cualitativas del coeficiente de Seebeck y de impedancia compleja. En estos materiales, el comportamiento eléctrico corresponde a semiconducción eléctrica extrínseca tipo-p. La conductividad eléctrica de los mismos es superior a la obtenida en disoluciones sólidas V-TiO2 y aumenta con la cantidad de dopantes introducida en la matriz de TiO2.
first_indexed 2024-12-10T22:57:39Z
format Article
id doaj.art-877180136661410088dd98869b2bf060
institution Directory Open Access Journal
issn 0366-3175
language English
last_indexed 2024-12-10T22:57:39Z
publishDate 2004-08-01
publisher Elsevier
record_format Article
series Boletín de la Sociedad Española de Cerámica y Vidrio
spelling doaj.art-877180136661410088dd98869b2bf0602022-12-22T01:30:13ZengElsevierBoletín de la Sociedad Española de Cerámica y Vidrio0366-31752004-08-01434792795Caracterización eléctrica de disoluciones sólidas (Cr,V,Ti)O<sub>2</sub> con estructura rutiloMonrós, G.Tena, M. A.Badenes, J. A.Benet, P.Calbo, J.Llusar, M.Sorlí, S.In this work (Cr,V,Ti)O2 solid solutions with rich-TiO2 compositions have been synthesized. Green samples and samples after each calcination have been characterized by X-Ray diffraction at room temperature, UV-V spectroscopy and electronic microscopy, in order to confirm the stability of these solid solutions with rutile-type structure at high temperatures (1400ºC). With the calcined samples at 1400ºC pellets were presses and Seebeck coefficient and complex impedance spectroscopy measurements were done. In these materials, the electrical behaviour corresponds to a extrinsic p-type semiconduction. The electrical conductivity is higher than that obtained in V-TiO2 solid solutions and it is enhanced with the amount of dopants in the TiO2 matrix.<br><br>En este estudio se han sintetizado disoluciones sólidas (Cr,V,Ti)O2 con composiciones ricas en TiO2. Las muestras, crudas y después de cada calcinación, se han caracterizado a temperatura ambiente por difracción de rayos X, espectroscopia UV-V y microscopía eléctronica para confirmar la estabilidad de estas disoluciones sólidas con estructura rutilo a altas temperaturas (1400 ºC). Se han prensado pastillas con las muestras calcinadas a 1400 ºC y con ellas se han realizado medidas cualitativas del coeficiente de Seebeck y de impedancia compleja. En estos materiales, el comportamiento eléctrico corresponde a semiconducción eléctrica extrínseca tipo-p. La conductividad eléctrica de los mismos es superior a la obtenida en disoluciones sólidas V-TiO2 y aumenta con la cantidad de dopantes introducida en la matriz de TiO2.http://ceramicayvidrio.revistas.csic.es/index.php/ceramicayvidrio/article/view/432/450ConductivityRutileVanadiumChromeConductividadRutiloVanadioCromo
spellingShingle Monrós, G.
Tena, M. A.
Badenes, J. A.
Benet, P.
Calbo, J.
Llusar, M.
Sorlí, S.
Caracterización eléctrica de disoluciones sólidas (Cr,V,Ti)O<sub>2</sub> con estructura rutilo
Boletín de la Sociedad Española de Cerámica y Vidrio
Conductivity
Rutile
Vanadium
Chrome
Conductividad
Rutilo
Vanadio
Cromo
title Caracterización eléctrica de disoluciones sólidas (Cr,V,Ti)O<sub>2</sub> con estructura rutilo
title_full Caracterización eléctrica de disoluciones sólidas (Cr,V,Ti)O<sub>2</sub> con estructura rutilo
title_fullStr Caracterización eléctrica de disoluciones sólidas (Cr,V,Ti)O<sub>2</sub> con estructura rutilo
title_full_unstemmed Caracterización eléctrica de disoluciones sólidas (Cr,V,Ti)O<sub>2</sub> con estructura rutilo
title_short Caracterización eléctrica de disoluciones sólidas (Cr,V,Ti)O<sub>2</sub> con estructura rutilo
title_sort caracterizacion electrica de disoluciones solidas cr v ti o sub 2 sub con estructura rutilo
topic Conductivity
Rutile
Vanadium
Chrome
Conductividad
Rutilo
Vanadio
Cromo
url http://ceramicayvidrio.revistas.csic.es/index.php/ceramicayvidrio/article/view/432/450
work_keys_str_mv AT monrosg caracterizacionelectricadedisolucionessolidascrvtiosub2subconestructurarutilo
AT tenama caracterizacionelectricadedisolucionessolidascrvtiosub2subconestructurarutilo
AT badenesja caracterizacionelectricadedisolucionessolidascrvtiosub2subconestructurarutilo
AT benetp caracterizacionelectricadedisolucionessolidascrvtiosub2subconestructurarutilo
AT calboj caracterizacionelectricadedisolucionessolidascrvtiosub2subconestructurarutilo
AT llusarm caracterizacionelectricadedisolucionessolidascrvtiosub2subconestructurarutilo
AT sorlis caracterizacionelectricadedisolucionessolidascrvtiosub2subconestructurarutilo