Ex Situ Examination of Matrix and Inclusions of API-X100 before and after Exposure to Bitumen at Elevated Temperature
The corrosivity of bitumen at 60 and 120 °C was examined by exposing American Petroleum Institute (API) X100 (yield strength 100 ksi, 690 MPa) pipeline steel to bitumen in an autoclave for 30 days. Prior to the autoclave measurements, the inclusion types in the API-X100 pipeline steel were character...
Main Authors: | , |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2021-09-01
|
Series: | Materials |
Subjects: | |
Online Access: | https://www.mdpi.com/1996-1944/14/17/5007 |
_version_ | 1797521108190101504 |
---|---|
author | Hongxing Liang Edouard Asselin |
author_facet | Hongxing Liang Edouard Asselin |
author_sort | Hongxing Liang |
collection | DOAJ |
description | The corrosivity of bitumen at 60 and 120 °C was examined by exposing American Petroleum Institute (API) X100 (yield strength 100 ksi, 690 MPa) pipeline steel to bitumen in an autoclave for 30 days. Prior to the autoclave measurements, the inclusion types in the API-X100 pipeline steel were characterized by scanning electron microscopy (SEM), and four types of inclusions were identified, according to their elemental compositions. The four types of inclusions and the surrounding matrix were characterized by ex situ SEM before and after exposure to bitumen. The results show that no obvious corrosion occured at the inclusions or the matrix after exposure at 60 and 120 °C. |
first_indexed | 2024-03-10T08:07:55Z |
format | Article |
id | doaj.art-8a313b8b461f42d29e28c96be3839775 |
institution | Directory Open Access Journal |
issn | 1996-1944 |
language | English |
last_indexed | 2024-03-10T08:07:55Z |
publishDate | 2021-09-01 |
publisher | MDPI AG |
record_format | Article |
series | Materials |
spelling | doaj.art-8a313b8b461f42d29e28c96be38397752023-11-22T10:54:55ZengMDPI AGMaterials1996-19442021-09-011417500710.3390/ma14175007Ex Situ Examination of Matrix and Inclusions of API-X100 before and after Exposure to Bitumen at Elevated TemperatureHongxing Liang0Edouard Asselin1Department of Materials Engineering, The University of British Columbia, Vancouver, BC V6T 1Z4, CanadaDepartment of Materials Engineering, The University of British Columbia, Vancouver, BC V6T 1Z4, CanadaThe corrosivity of bitumen at 60 and 120 °C was examined by exposing American Petroleum Institute (API) X100 (yield strength 100 ksi, 690 MPa) pipeline steel to bitumen in an autoclave for 30 days. Prior to the autoclave measurements, the inclusion types in the API-X100 pipeline steel were characterized by scanning electron microscopy (SEM), and four types of inclusions were identified, according to their elemental compositions. The four types of inclusions and the surrounding matrix were characterized by ex situ SEM before and after exposure to bitumen. The results show that no obvious corrosion occured at the inclusions or the matrix after exposure at 60 and 120 °C.https://www.mdpi.com/1996-1944/14/17/5007API-X100 pipelinebitumencorrosioninclusion |
spellingShingle | Hongxing Liang Edouard Asselin Ex Situ Examination of Matrix and Inclusions of API-X100 before and after Exposure to Bitumen at Elevated Temperature Materials API-X100 pipeline bitumen corrosion inclusion |
title | Ex Situ Examination of Matrix and Inclusions of API-X100 before and after Exposure to Bitumen at Elevated Temperature |
title_full | Ex Situ Examination of Matrix and Inclusions of API-X100 before and after Exposure to Bitumen at Elevated Temperature |
title_fullStr | Ex Situ Examination of Matrix and Inclusions of API-X100 before and after Exposure to Bitumen at Elevated Temperature |
title_full_unstemmed | Ex Situ Examination of Matrix and Inclusions of API-X100 before and after Exposure to Bitumen at Elevated Temperature |
title_short | Ex Situ Examination of Matrix and Inclusions of API-X100 before and after Exposure to Bitumen at Elevated Temperature |
title_sort | ex situ examination of matrix and inclusions of api x100 before and after exposure to bitumen at elevated temperature |
topic | API-X100 pipeline bitumen corrosion inclusion |
url | https://www.mdpi.com/1996-1944/14/17/5007 |
work_keys_str_mv | AT hongxingliang exsituexaminationofmatrixandinclusionsofapix100beforeandafterexposuretobitumenatelevatedtemperature AT edouardasselin exsituexaminationofmatrixandinclusionsofapix100beforeandafterexposuretobitumenatelevatedtemperature |