Ex Situ Examination of Matrix and Inclusions of API-X100 before and after Exposure to Bitumen at Elevated Temperature
The corrosivity of bitumen at 60 and 120 °C was examined by exposing American Petroleum Institute (API) X100 (yield strength 100 ksi, 690 MPa) pipeline steel to bitumen in an autoclave for 30 days. Prior to the autoclave measurements, the inclusion types in the API-X100 pipeline steel were character...
Main Authors: | Hongxing Liang, Edouard Asselin |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2021-09-01
|
Series: | Materials |
Subjects: | |
Online Access: | https://www.mdpi.com/1996-1944/14/17/5007 |
Similar Items
-
The Corrosion Behavior of X100 Pipeline Steel in a Sodium Chloride Solution Containing Magnesium and Calcium
by: Xiaoning Yang, et al.
Published: (2023-07-01) -
Three phase corrosion of pipeline steel: Size effects of deposited solids under water droplets and an oil diffusion barrier
by: Hongxing Liang, et al.
Published: (2021-03-01) -
Bitumen safety code /
by: 685 Institute of Petroleum (Great Britain)
Published: (1991) -
Saturated bitumen felts
by: 982 SIRIM -
The Shell Bitumen handbook /
by: Read, John, 1968-, et al.
Published: (2003)