Reduction Smelting Low Ferronickel from Pre-concentrated Nickel-Iron Ore of Nickel Laterite
The research of smelting low ferronickel from pre-concentrate nickel-iron ore with 2.76 % Ni and 38.00 % Fetotal was carried out to find an effective way for stainless steel enterprises to use the low-nickel laterite reasonable. The results show that Ni and Fe both have a certain degree of enrichmen...
Main Authors: | Zhu Deqing, Zhou Xianlin, Luo Yanhong, Pan Jian, Bai Bing |
---|---|
Format: | Article |
Language: | English |
Published: |
De Gruyter
2016-11-01
|
Series: | High Temperature Materials and Processes |
Subjects: | |
Online Access: | https://doi.org/10.1515/htmp-2015-0025 |
Similar Items
-
Smelting of low-grade saprolitic nickel ore in DC-arc furnace
by: Nurjaman F., et al.
Published: (2023-01-01) -
High-Grade Ferronickel Concentrates Prepared from Laterite Nickel Ore by a Carbothermal Reduction and Magnetic Separation Method
by: Jingzhe Zhang, et al.
Published: (2023-11-01) -
Use of colemanite in ferronickel smelting
by: Keskinkilic E., et al.
Published: (2019-01-01) -
Phases transformation of nickel lateritic ore during dehydration
by: Huang Q., et al.
Published: (2011-01-01) -
The Nickel Production Methods from Laterites and the Greek Ferronickel Production among Them
by: Emmanouil N. Zevgolis, et al.
Published: (2022-01-01)