LONGITUDINAL DIFFERENT-WALL OF HOLLOW CASTINGS AT FORMING OF INTERNAL SURFACE OUT OF MELT WITHOUT APPLICATION OF ROD
The reasons of occurrence of axial polythickness of hollow slugs at forming of internal surface of melt without application of stick are investigated. The ways of its minimization are determined.
Main Authors: | E. I. Marukovich, V. F. Bevza, V. P. Grusha |
---|---|
Format: | Article |
Language: | English |
Published: |
Belarusian National Technical University
2006-05-01
|
Series: | Litʹë i Metallurgiâ |
Online Access: | https://lim.bntu.by/jour/article/view/1559 |
Similar Items
-
HARDENING OF CASTINGS AT FREE FORMING OF INTERNAL SURFACE
by: E. I. Marukovich, et al.
Published: (2005-08-01) -
PRINCIPALLY NEW EFFECTIVE CASTING PROCESS OF THE HOLLOW CYLINDRICAL SLUGS OF CAST IRON BY METHOD OF DIRECTIONAL SOLIDIFICATION
by: E. I. Marukovich, et al.
Published: (2010-08-01) -
THEORETICAL AND TECHNOLOGICAL BASIS OF CASTING OF HOLLOW BILLETS BY THE METHOD OF DIRECTIONAL SOLIDIFICATION
by: E. I. Marukovich, et al.
Published: (2011-05-01) -
CONTINUOUSLY AND CYCLIC CASTING BY SILVERING OF PIPE SLUGS
by: E. I. Marukovich, et al.
Published: (2014-03-01) -
TECHNOLOGICAL PARAMETERS OF SLUGS CASTING OF GREY CAST IRON BY FROSTING
by: E. I. Marukovich, et al.
Published: (2009-08-01)