Analysis of impact toughness and the critical stress intensity factor KIc in ferrite-austenite welded joints with different heat input
Introduction/purpose: Constructions always have several critical points that can be sources of possible defects. All these critical places must be taken into account in safety assessment where the most unfavorable exploitation factors are considered and the local safety of a joint is assessed. To...
Main Authors: | Aleksandar G. Bukvić, Dalibor P. Petrović, Igor Z. Radisavljević, Saša S. Dimitrić |
---|---|
Format: | Article |
Language: | English |
Published: |
University of Defence in Belgrade
2023-04-01
|
Series: | Vojnotehnički Glasnik |
Subjects: | |
Online Access: | https://scindeks.ceon.rs/article.aspx?artid=0042-84692302392B |
Similar Items
-
Influence of heat input on the tensile properties of austenitic-ferritic welded joints
by: Aleksandar G. Bukvić, et al.
Published: (2022-04-01) -
Measurement uncertainty of plane-strain fracture toughness KIC testing by the Monte Carlo Method
by: Daniel Antonio Kapper Fabricio, et al. -
Light curve solutions and out-of-eclipse variability of KIC 10031409, KIC 11228612, KIC 11403216 and KIC 11913071
by: Kjurkchieva D., et al.
Published: (2017-01-01) -
Tensile properties of shielded metal arc welded dissimilar joints of nuclear grade ferritic steel and austenitic stainless steel
by: Karthick K., et al.
Published: (2016-12-01) -
The influence of the heat treatment on delta ferrite transformation in austenitic stainless steel welds
by: B. Mateša, et al.
Published: (2012-04-01)