Highly Enhanced Hot Ductility Performance of Advanced SA508-4N RPV Steel by Trace Impurity Phosphorus and Rare Earth Cerium
Advanced SA508-4N RPV steel samples, unadded, P-added, and P+Ce-added, are investigated on their hot ductility behavior. Hot tensile tests are carried out in the temperature range of 750 to 1000 °C through a Gleeble 1500D machine. It is demonstrated that the deformation temperatures of all the three...
Main Authors: | Yu Guo, Yu Zhao, Shenhua Song |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2020-11-01
|
Series: | Metals |
Subjects: | |
Online Access: | https://www.mdpi.com/2075-4701/10/12/1598 |
Similar Items
-
A comparative study of hot ductility of unadded and Ce-added SA508-4N RPV steels
by: Yu Guo, et al.
Published: (2020-11-01) -
Quantitative dependence of ductile-to-brittle transition on phosphorus grain boundary segregation for a novel Ni–Cr–Mo RPV steel
by: Kai Wang, et al.
Published: (2021-11-01) -
Relation of embrittlement to phosphorus grain-boundary segregation for an advanced Ni–Cr–Mo RPV steel
by: Yu Guo, et al.
Published: (2022-05-01) -
Effects of B on the Hot Ductility of Fe-36Ni Invar Alloy
by: Zheng Yaxu, et al.
Published: (2019-02-01) -
Effect of Sulfur on Antimony-Induced High-Temperature Ductility Deterioration of C-Mn Steel
by: Guilin Sun, et al.
Published: (2023-01-01)