Piercing and Surface-Crack Defects in Cold Combined Forward-Backward Extrusion

Metal flow tends to be complex and difficult to predict in the combined forward-backward extrusion (CFBE) process. Piercing and surface-crack defects are phenomenal in forming fasteners featuring a forward extruded pin and a backward extruded cup. In this work, a series of the CFBE tests with variou...

Full description

Bibliographic Details
Main Authors: Heng-Sheng Lin, Chien-Yu Lee, Wen-Shun Li
Format: Article
Language:English
Published: MDPI AG 2021-04-01
Series:Applied Sciences
Subjects:
Online Access:https://www.mdpi.com/2076-3417/11/9/3900
Description
Summary:Metal flow tends to be complex and difficult to predict in the combined forward-backward extrusion (CFBE) process. Piercing and surface-crack defects are phenomenal in forming fasteners featuring a forward extruded pin and a backward extruded cup. In this work, a series of the CFBE tests with various combinations of the forward extrusion ratio (FER) and the backward extrusion ratio (BER) were conducted. A forming limit diagram, detailed with the piercing and surface-crack defects on the forward extruded pin or the backward extruded cup, was developed to provide a conception in choosing appropriate extrusion ratios in forming fasteners with such pin-and-cup features. With the aid of the forming load-stroke curves and the finite element analysis of fracture damage, the fracturing mechanism for the CFBE process was provided.
ISSN:2076-3417