The hot flow behavior of Al-2wt.%Cu-1wt.%Mn alloy based on Gleebe-3800 hot compression simulation
Flow behavior of Al-2.0wt.%Cu-1.0wt.%Mn aluminum alloy was investigated by hot compressive test using a Gleebe-3800 thermal simulator. The test parameters about temperature and strain rate range from 573K to 773 K and from 0.01s-1 to 5s-1, respectively, and the true strain is up to 0.6. It can be se...
Main Authors: | Chen JinLong, Liao Hengcheng, Xu Heting |
---|---|
Format: | Article |
Language: | English |
Published: |
EDP Sciences
2018-01-01
|
Series: | MATEC Web of Conferences |
Online Access: | https://doi.org/10.1051/matecconf/201820703016 |
Similar Items
-
Microstructure and Hot Deformation Behavior of the Mg–8 wt.% Sn–1.5 wt.% Al Alloy
by: Zhaoqian Sun, et al.
Published: (2021-04-01) -
Flow Behavior Characteristics and Processing Map of Fe-6.5wt. %Si Alloys during Hot Compression
by: Shibo Wen, et al.
Published: (2018-03-01) -
Investigations on Microstructure and Properties of 16 wt% Cr-3 wt% B-0.6 wt% C-1 wt% Mn-Fe Alloy
by: Jiawei Ding, et al.
Published: (2018-07-01) -
Flow behavior and microstructure evolution of Al-3.65Cu-0.98Li (wt%) alloy during hot deformation
by: Hai-tao Lin, et al.
Published: (2022-01-01) -
Simultaneous Increase of Electrical Conductivity and Hardness of Al–1.5 wt.% Mn Alloy by Addition of 1.5 wt.% Cu and 0.5 wt.% Zr
by: Nikolay Belov, et al.
Published: (2019-11-01)