Bonding performance of universal adhesives with concomitant use of silanes to CAD/CAM blocks

ABSTRACT Objective: This study assessed whether the use of a silane coupling agent influence the bond strength of two universal adhesives to ceramic or resin CAD/CAM blocks. Methods: Forty-eight samples were obtained from each resin nano-ceramic hybrid block (RCBs) and lithium disilicate ceramic b...

Full description

Bibliographic Details
Main Authors: Marina AMARAL, Jaqueline Maria Brandão RIZZATO, Victoria Caroline Souza de ALMEIDA, Priscila Christiane Suzy LIPORONI, Rayssa Ferreira ZANATTA
Format: Article
Language:English
Published: Faculdade São Leopoldo Mandic 2023-06-01
Series:RGO: Revista Gaúcha de Odontologia
Subjects:
Online Access:http://www.scielo.br/scielo.php?script=sci_arttext&pid=S1981-86372023000100311&lng=en&tlng=en
_version_ 1797792695274438656
author Marina AMARAL
Jaqueline Maria Brandão RIZZATO
Victoria Caroline Souza de ALMEIDA
Priscila Christiane Suzy LIPORONI
Rayssa Ferreira ZANATTA
author_facet Marina AMARAL
Jaqueline Maria Brandão RIZZATO
Victoria Caroline Souza de ALMEIDA
Priscila Christiane Suzy LIPORONI
Rayssa Ferreira ZANATTA
author_sort Marina AMARAL
collection DOAJ
description ABSTRACT Objective: This study assessed whether the use of a silane coupling agent influence the bond strength of two universal adhesives to ceramic or resin CAD/CAM blocks. Methods: Forty-eight samples were obtained from each resin nano-ceramic hybrid block (RCBs) and lithium disilicate ceramic blocks (LD). Samples were treated with silane with MDP (Monobond - S-MDP), silane without MDP (Prosil - PS), and no silane application (Control - Ctr) followed by universal adhesive with silane (UAS) and without silane (UA) (n=8). Three polyurethane tubes (1.5 mm of internal diameter) were positioned in each sample treated surface and filled with a dual cured resin cement. Bond strength was assessed by microshear bond strength test and failure analysis was performed for all samples. Results: For the RCBs, UAS presented the highest bond strength values (p=0.004). Silane application was not significant in bond strength values (p=0.444). For LD, silane application was significant in bond strength values (p<0.001), but the adhesive was not (p=0.066). Failure analysis showed high prevalence of adhesive failures for both substrates. Conclusion: A silane-containing universal adhesive promoted the best bond strength results to the resin nano-ceramic hybrid block. For bonding to a glass-ceramic CAD/CAM material, additional silane (without MDP) application presented the best results.
first_indexed 2024-03-13T02:37:36Z
format Article
id doaj.art-a0a69d7cd4554c29ba3ac5625df999a1
institution Directory Open Access Journal
issn 1981-8637
language English
last_indexed 2024-03-13T02:37:36Z
publishDate 2023-06-01
publisher Faculdade São Leopoldo Mandic
record_format Article
series RGO: Revista Gaúcha de Odontologia
spelling doaj.art-a0a69d7cd4554c29ba3ac5625df999a12023-06-28T23:17:16ZengFaculdade São Leopoldo MandicRGO: Revista Gaúcha de Odontologia1981-86372023-06-017110.1590/1981-86372023002020220004Bonding performance of universal adhesives with concomitant use of silanes to CAD/CAM blocksMarina AMARALhttps://orcid.org/0000-0002-4301-2760Jaqueline Maria Brandão RIZZATOhttps://orcid.org/0000-0001-5936-6152Victoria Caroline Souza de ALMEIDAhttps://orcid.org/0000-0003-2781-1105Priscila Christiane Suzy LIPORONIhttps://orcid.org/0000-0001-6787-1167Rayssa Ferreira ZANATTAhttps://orcid.org/0000-0001-5230-1508ABSTRACT Objective: This study assessed whether the use of a silane coupling agent influence the bond strength of two universal adhesives to ceramic or resin CAD/CAM blocks. Methods: Forty-eight samples were obtained from each resin nano-ceramic hybrid block (RCBs) and lithium disilicate ceramic blocks (LD). Samples were treated with silane with MDP (Monobond - S-MDP), silane without MDP (Prosil - PS), and no silane application (Control - Ctr) followed by universal adhesive with silane (UAS) and without silane (UA) (n=8). Three polyurethane tubes (1.5 mm of internal diameter) were positioned in each sample treated surface and filled with a dual cured resin cement. Bond strength was assessed by microshear bond strength test and failure analysis was performed for all samples. Results: For the RCBs, UAS presented the highest bond strength values (p=0.004). Silane application was not significant in bond strength values (p=0.444). For LD, silane application was significant in bond strength values (p<0.001), but the adhesive was not (p=0.066). Failure analysis showed high prevalence of adhesive failures for both substrates. Conclusion: A silane-containing universal adhesive promoted the best bond strength results to the resin nano-ceramic hybrid block. For bonding to a glass-ceramic CAD/CAM material, additional silane (without MDP) application presented the best results.http://www.scielo.br/scielo.php?script=sci_arttext&pid=S1981-86372023000100311&lng=en&tlng=enAcid etchingCeramicsComputer-aided designSilanes
spellingShingle Marina AMARAL
Jaqueline Maria Brandão RIZZATO
Victoria Caroline Souza de ALMEIDA
Priscila Christiane Suzy LIPORONI
Rayssa Ferreira ZANATTA
Bonding performance of universal adhesives with concomitant use of silanes to CAD/CAM blocks
RGO: Revista Gaúcha de Odontologia
Acid etching
Ceramics
Computer-aided design
Silanes
title Bonding performance of universal adhesives with concomitant use of silanes to CAD/CAM blocks
title_full Bonding performance of universal adhesives with concomitant use of silanes to CAD/CAM blocks
title_fullStr Bonding performance of universal adhesives with concomitant use of silanes to CAD/CAM blocks
title_full_unstemmed Bonding performance of universal adhesives with concomitant use of silanes to CAD/CAM blocks
title_short Bonding performance of universal adhesives with concomitant use of silanes to CAD/CAM blocks
title_sort bonding performance of universal adhesives with concomitant use of silanes to cad cam blocks
topic Acid etching
Ceramics
Computer-aided design
Silanes
url http://www.scielo.br/scielo.php?script=sci_arttext&pid=S1981-86372023000100311&lng=en&tlng=en
work_keys_str_mv AT marinaamaral bondingperformanceofuniversaladhesiveswithconcomitantuseofsilanestocadcamblocks
AT jaquelinemariabrandaorizzato bondingperformanceofuniversaladhesiveswithconcomitantuseofsilanestocadcamblocks
AT victoriacarolinesouzadealmeida bondingperformanceofuniversaladhesiveswithconcomitantuseofsilanestocadcamblocks
AT priscilachristianesuzyliporoni bondingperformanceofuniversaladhesiveswithconcomitantuseofsilanestocadcamblocks
AT rayssaferreirazanatta bondingperformanceofuniversaladhesiveswithconcomitantuseofsilanestocadcamblocks