Natural hydrolytic ageing of PA6 and bio-reinforced composites
Hydrolytic ageing or hydrolysis is the destruction of chemical bonds by the action of water. Among the polymers most affected by hydrolysis are the polyamides, since PA6 is hygroscopic, due to the amide groups. PA6 with its interesting technical applications could be found in humid environments, whi...
Main Authors: | Oulidi Oumayma, Nakkabi Asmae, Fahim Mohammed, Elmoualij Noureddine |
---|---|
Format: | Article |
Language: | English |
Published: |
EDP Sciences
2022-01-01
|
Series: | MATEC Web of Conferences |
Online Access: | https://www.matec-conferences.org/articles/matecconf/pdf/2022/07/matecconf_ndecs22_00008.pdf |
Similar Items
-
Incorporation of olive pomace as a natural filler in to the PA6 matrix: Effect on the structure and thermal properties of synthetic Polyamide 6
by: Oumayma Oulidi, et al.
Published: (2022-11-01) -
Enhancing and hindering biodegradation: A comparative study on polyamide 6 reinforced with bio-fillers (peanut shell, olive pomace, and plaster)
by: Oumayma Oulidi, et al.
Published: (2024-09-01) -
Peanut shell from agricultural wastes as a sustainable filler for polyamide biocomposites fabrication
by: Oumayma Oulidi, et al.
Published: (2022-08-01) -
Biodegradation of polyamide 6 by Lysinibacillus sp, Alcaligene faecalis and Enterococcus faecalis
by: Oumayma Oulidi, et al.
Published: (2022-09-01) -
Impact of peanut shells, olive pomace, and plaster on the dielectric properties of PA6
by: O. Oulidi, et al.
Published: (2023-12-01)