Precipitation behavior of a new Cu-Ni-Co-Si-Fe-Mg alloy designed with low cobalt content
A new Cu-1.5Ni-0.7Co-0.7Si-0.3Fe-0.1Mg alloy with low cobalt content was designed. Multi-stage thermo-mechanical treatment (MTT) was used to produce the high-performance alloy with hardness of 286 HV, yield strength of 858 MPa, tensile strength of 910 MPa and electrical conductivity of 45.4 % IACS....
Main Authors: | Liu-xin Qin, Tao Zhou, Xu Wang, Yan-bin Jiang, Feng Liu, Zhu Xiao, Qian Lei, Yan-lin Jia, Yi Luo, Zhou Li |
---|---|
Format: | Article |
Language: | English |
Published: |
Elsevier
2024-04-01
|
Series: | Materials & Design |
Subjects: | |
Online Access: | http://www.sciencedirect.com/science/article/pii/S0264127524002053 |
Similar Items
-
Investigation of Microstructure and Wear Properties of Precipitates-Strengthened Cu-Ni-Si-Fe Alloy
by: Chun-Hao Peng, et al.
Published: (2023-01-01) -
Study on aging strengthening and nano precipitates of Cu–Ni–Mn–Fe alloy
by: Juntao Zou, et al.
Published: (2020-01-01) -
Characterizations on Precipitations in the Cu-Rich Corner of Cu-Ni-Al Ternary Phase Diagram
by: Yongxin Zhou, et al.
Published: (2023-02-01) -
Effect of V Addition on Microstructure and Properties of Cu-1.6Ni-1.2Co-0.65Si Alloys
by: Jinfeng Zou, et al.
Published: (2019-06-01) -
The strengthening role of micro-sized phases and nano-precipitates in Al–Mg2Si–Cu(–Ni) alloys at 25 °C and 350 °C
by: Yilin Sun, et al.
Published: (2023-05-01)