Transport evidence of mass-less Dirac fermions in (Cd1−x−yZnxMny)3As2 (x + y = 0.4)

Charge carriers parameters on a 2D-layer surface for (Cd _1−x−y Zn _x Mn _y ) _3 As _2 ( y  = 0.08) (the concentration ${n}_{2D}$  = 1.9 × 10 ^12 cm ^–2 , the effective value of the 2D-layer ${d}_{2D}={n}_{2D}/{n}_{3D}$  = 14.5 nm, the wave vector ${k}_{F}$  = 0.1 nm ^–1 , the charge carriers relaxa...

Full description

Bibliographic Details
Main Authors: V S Zakhvalinskii, T B Nikulicheva, E A Pilyuk, E Lähderanta, M A Shakhov, O N Ivanov, E P Kochura, A V Kochura, B A Aronzon
Format: Article
Language:English
Published: IOP Publishing 2020-01-01
Series:Materials Research Express
Subjects:
Online Access:https://doi.org/10.1088/2053-1591/ab688b
Description
Summary:Charge carriers parameters on a 2D-layer surface for (Cd _1−x−y Zn _x Mn _y ) _3 As _2 ( y  = 0.08) (the concentration ${n}_{2D}$  = 1.9 × 10 ^12 cm ^–2 , the effective value of the 2D-layer ${d}_{2D}={n}_{2D}/{n}_{3D}$  = 14.5 nm, the wave vector ${k}_{F}$  = 0.1 nm ^–1 , the charge carriers relaxation time due to dispersion ${\tau }_{D}$  = 1.8 × 10 ^–13 s, the velocity of charge carriers on Fermi surface ${v}_{F}=\hslash {k}_{F}/{m}_{c}$  = 2.6 ^5  × 10 ^5 m s ^−1 , the mean free path ${l}_{F}={v}_{F}{\tau }_{D}$  = 47.7 nm) were determined. It was found that the dependence of the cyclotron m ass m _с (0)/m _0 on Fermi wave vector k _F for (Cd _1−x−y Zn _x Mn _y ) _3 As _2 ( y  = 0.08) is in compliance with a theoretical linear dependence, that describes mass-less Dirac fermions.