Fatigue behaviour of a glass coating on Ti6AL4V for biomedical applications
The fixation of bone replacement implants to the hosting tissue can be improved if the implants have a bioactive surface that can precipitate hydroxyapatite in vivo. Titanium alloys, despite their desirable mechanical and nontoxic properties, are not bioactive and, therefore, do not bond directly t...
Main Authors: | Juan José Pavón, E. Jiménez-Piqué, M. Anglada, E. Saiz, A. P. Tomsia |
---|---|
Format: | Article |
Language: | English |
Published: |
Universidad de Antioquia
2006-08-01
|
Series: | Revista Facultad de Ingeniería Universidad de Antioquia |
Subjects: | |
Online Access: | https://revistas.udea.edu.co/index.php/ingenieria/article/view/343446 |
Similar Items
-
Determination of the Pressure Dependence of Raman Mode for an Alumina–Glass Pair in Hertzian Contact
by: Karl Delbé, et al.
Published: (2022-12-01) -
Fatigue behaviour of a glass coating
on Ti6AL4V for biomedical applications
by: Juan José Pavón, et al.
Published: (2006-01-01) -
Hertzian Load-bearing Capacity of Hybrid and Nano-hybrid Resin Composites Stored Dry and Wet
by: Farmani S, et al.
Published: (2016-03-01) -
Surface mechanical analyses by Hertzian indentation Análises mecânicas de superfície via indentação Hertzian
by: A. Franco Jr., et al.
Published: (2004-06-01) -
Novel Ni-P-Tribaloy Composite Protective Coating
by: Ahmed Mabrouk, et al.
Published: (2023-05-01)