INFLUENCE OF THE INDUCTION HEAT ON STRUCTURE FORMATION AT RECRYSTALLIZATION ANNEALING OF THE CIRCULAR ROLLED STEEL

There are studied the peculiarities of structure formation at crystallization expression using induction heat by currents with frequency 2400 and 8000 Hz of rod iron with diameter 16-40 mm from steels 35,40 and 40X. It is determined that single induction heat during 2-5 minutes provides required str...

Full description

Bibliographic Details
Main Authors: P. S. Gurchenko, A. I. Mihluk
Format: Article
Language:English
Published: Belarusian National Technical University 2004-02-01
Series:Litʹë i Metallurgiâ