Low-cycle fatigue behaviors of 316L austenitic stainless steel in high temperature water: Effects of pre-soaking, dissolved oxygen, and boric acid & lithium hydroxide

Latest studies found that for 316LN austenitic stainless steel (ASS), its LCF life decreased noticeably in high temperature water containing a great amount of dissolved oxygen (DO) (2 ppm DO), compared with that in the water containing 50 or 100 ppb DO. This finding is different from previous studie...

Descrición completa

Detalles Bibliográficos
Main Authors: Yida Xiong, Yutaka Watanabe, Yuki Shibayama, Xiangyu Zhong, Nicolas Mary
Formato: Artigo
Idioma:English
Publicado: Elsevier 2022-09-01
Series:Nuclear Engineering and Technology
Subjects:
Acceso en liña:http://www.sciencedirect.com/science/article/pii/S1738573322001887