Low-cycle fatigue behaviors of 316L austenitic stainless steel in high temperature water: Effects of pre-soaking, dissolved oxygen, and boric acid & lithium hydroxide

Latest studies found that for 316LN austenitic stainless steel (ASS), its LCF life decreased noticeably in high temperature water containing a great amount of dissolved oxygen (DO) (2 ppm DO), compared with that in the water containing 50 or 100 ppb DO. This finding is different from previous studie...